Scope
1.1 Form:This specification covers a corrosion and heat-resistant nickel alloy in the form of bars, forgings,flash welded rings, and stock for forging or flash welded rings.1.2 Application:These products have been used typically for parts requiring high resistance to creep andstress-rupture up to 1300 °F (704 °C) and oxidation resistance up to 1800 °F (982 °C), but usage isnot limited to such applications.

SAE AMS5663M-2004 Referenced Document

  • ASTM E10 Standard Test Method for Brinell Hardness of Metallic Materials*2023-08-03 Update
  • ASTM E103 Standard Test Method for Rapid Indentation Hardness Testing of Metallic Materials
  • ASTM E112 Standard Test Methods for Determining Average Grain Size
  • ASTM E139 Standard Test Methods for Conducting Creep, Creep-Rupture, and Stress-Rupture Tests of Metallic Materials*2018-10-01 Update
  • ASTM E21 Standard Test Methods for Elevated Temperature Tension Tests of Metallic Materials
  • ASTM E292 Standard Test Methods for Conducting Time-for-Rupture Notch Tension Tests of Materials
  • ASTM E354 Standard Test Methods for Chemical Analysis of High-Temperature, Electrical, Magnetic, and Other Similar Iron, Nickel, and Cobalt Alloys
  • ASTM E8 Standard Test Methods for Tension Testing of Metallic Materials
  • ASTM E8M Standard Test Methods for Tension Testing of Metallic Materials [Metric] *2024-04-20 Update
  • SAE AMS2261 TOLERANCES Nickel and Nickel Base Alloy Bars
  • SAE AMS2269 CHEMICAL CHECK ANALYSIS LIMITS Wrought Nickel and Nickel Base Alloys
  • SAE AMS2371 QUALITY ASSURANCE SAMPLING OF CORROSION AND HEAT RESISTANT ALLOYS Wrought Products and Forging Stock
  • SAE AMS2374 QUALITY ASSURANCE SAMPLING OF CORROSION AND HEAT RESISTANT STEELS AND ALLOYS Forgings and Forging Stock
  • SAE AMS2750 PYROMETRY
  • SAE AMS2806 IDENTIFICATION Bars, Wire, Mechanical Tubing, and Extrusions Carbon and Alloy Steels and Heat and Corrosion Resistant Steels and Alloys
  • SAE AMS2808 IDENTIFICATION Forgings
  • SAE AMS7490 RINGS, FLASH WELDED Corrosion and Heat Resistant
  • SAE ARP1313 DETERMINATION OF TRACE ELEMENTS IN HIGH TEMPERATURE ALLOYS

SAE AMS5663M-2004 history

  • 1970 SAE AMS5663P-2022 Nickel Alloy, Corrosion- and Heat-Resistant, Bars, Forgings, Rings, and Stock for Forgings and Rings, 52.5Ni - 19Cr - 3.0Mo - 5.1Cb (Nb) - 0.90Ti - 0.50Al - 18Fe, Consumable Electrode or Vacuum Induction Melted, 1775 °F (968 °C) Solution
  • 2016 SAE AMS5663N-2016 Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 52.5Ni - 19Cr - 3.0Mo - 5.1Cb (Nb) - 0.90Ti - 0.50Al - 18Fe Consumable Electrode or Vacuum Induction Melted 1775 °F (968 °C) Solution and Precipitation Heat Treated
  • 2009 SAE AMS5663M-2009 Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 52.5Ni - 19Cr - 3.0Mo - 5.1Cb (Nb) - 0.90Ti - 0.50Al - 18Fe Consumable Electrode or Vacuum Induction Melted 1775 °F (968 °C) Solution and Precipitation Heat Treated (Composition similar
  • 2004 SAE AMS5663M-2004 Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 52.5Ni 19Cr 3.0Mo 5.1Cb (Nb) 0.90Ti 0.50Al 19Fe Consumable Electrode or Vacuum Induction Melted 1775°F (968°C) Solution and Precipitation Heat Treated
  • 2003 SAE AMS5663L-2003 Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 52.5Ni - 19Cr - 3.0Mo - 5.1Cb - 0.90Ti - 0.50Al - 18Fe Consumable Electrode or Vacuum Induction Melted 1775 Degrees F (968 Degrees C) Solution and Precipitation Heat Treated UNS N0
  • 2002 SAE AMS5663K-2002 Nickel Alloy@ Corrosion and Heat-Resistant@ Bars@ Forgings@ and Rings 52.5Ni - 19Cr - 3.0Mo - 5.1Cb - 0.90Ti - 0.50Al - 18Fe Consumable Electrode or Vacuum Induction Melted 1775 °F (968 °C) Solution and Precipitation Heat Treated (UNS N07718)
  • 1997 SAE AMS5663J-1997 Nickel Alloy@ Corrosion and Heat Resistant@ Bars@ Forgings@ and Rings 52.5Ni - 19Cr - 3.0Mo - 5.1Cb - 0.90Ti - 0.50Al - 18Fe Consumable Electrode or Vacuum Induction Melted 1775 Degrees F (968 Degrees C) Solution and Precipitation Heat Treated (UNS N07718
  • 1996 SAE AMS5663H-1996 Nickel Alloy@ Corrosion & Heat Resistant@ Bars@ Forgings@ and Rings 52.5Ni - 19Cr - 3.0Mo - 5.1Cb - 0.90Ti - 0.50Al - 19Fe Consumable Electrode or Vacuum Induction Melted 1775 Degrees F (968 Degrees C) Solution and Precipitation Heat Treated (UNS N07718)
  • 1989 SAE AMS5663G-1989 ALLOY BARS, FORGINGS, AND RINGS, CORROSION AND HEAT RESISTANT 52.5Ni - 19Cr - 3.0Mo - 5.1(Cb + Ta) - 0.90Ti - 0.50Al - 19Fe Consumable Electrode or Vacuum Induction Melted 1775°F (968°C) Solution and Precipitation Heat Treated
  • 1989 SAE AMS5663F-1989 ALLOY BARS@ FORGINGS@ AND RINGS@ CORROSION AND HEAT RESISTANT 52.5Ni - 19Cr - 3.0Mo - 5.1(Cb + Ta) - 0.90Ti - 0.50Al - 19Fe Consumable Electrode or Vacuum Induction Melted 1750°F (955°C) Solution and Precipitation Heat Treated (UNS N07718)
  • 1987 SAE AMS5663E-1987 ALLOY BARS@ FORGINGS@ AND RINGS@ CORROSION AND HEAT RESISTANT 52.5Ni - 19Cr - 3.0Mo - 5.1(Cb + Ta) - 0.90Ti - 0.50Al - 19Fe Consumable Electrode or Vacuum Induction Melted 1750°F (955°C) Solution and Precipitation Heat Treated (UNS N07718)
  • 1980 SAE AMS5663D-1980 ALLOY BARS, FORGINGS, AND RINGS, CORROSION AND HEAT RESISTANT 52.5Ni - 19Cr - 3.0Mo - 5.1(Cb + Ta) - 0.90Ti - 0.50Al - 19Fe Consumable Electrode or Vacuum Induction Melted 1750°F (955°C) Solution and Precipitation Heat Treated
  • 1972 SAE AMS5663C-1972 ALLOY BARS, FORGINGS, AND RINGS, CORROSION AND HEAT RESISTANT Nickel Base - 19Cr - 3.1Mo - 5.1(Cb + Ta) - 0.90Ti - 0.50Al - 19Fe Consumable Electrode or Vacuum Induction Melted 1750 F (954.4 C) Solution and Precipitation Heat Treated
  • 1967 SAE AMS5663B-1967 ALLOY BARS, FORGINGS, AND RINGS, CORROSION AND HEAT RESISTANT Nickel Base - 19Cr - 3.1Mo - 5.1(Cb + Ta) - 0.90Ti - 0.50Al Consumable Electrode or Vacuum Induction Melted 1750 F (954.4 C) Solution and Precipitation Heat Treated
  • 1966 SAE AMS5663A-1966 ALLOY BARS, FORGINGS, AND RINGS, CORROSION AND HEAT RESISTANT Nickel Base - 19Cr - 3.1Mo - 5.1(Cb + Ta) - 0.90Ti - 0.50Al Solution and Precipitation Heat Treated Consumable Electrode or Vacuum Induction Melted
  • 1965 SAE AMS5663-1965 ALLOY BARS, FORGINGS, AND RINGS, CORROSION AND HEAT RESISTANT Nickel Base - 19Cr - 3.1Mo - 5.1(Cb + Ta) - 0.90Ti - 0.50Al Solution and Precipitation Heat Treated Consumable Electrode or Vacuum Induction Melted



Copyright ©2024 All Rights Reserved