SAE AMS5663A-1966
ALLOY BARS, FORGINGS, AND RINGS, CORROSION AND HEAT RESISTANT Nickel Base - 19Cr - 3.1Mo - 5.1(Cb + Ta) - 0.90Ti - 0.50Al Solution and Precipitation Heat Treated Consumable Electrode or Vacuum Induction Melted

Standard No.
SAE AMS5663A-1966
Release Date
1966
Published By
Society of Automotive Engineers (SAE)
Status
Replace By
SAE AMS5663B-1967
Latest
SAE AMS5663P-2022

SAE AMS5663A-1966 history

  • 1970 SAE AMS5663P-2022
  • 2016 SAE AMS5663N-2016 Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 52.5Ni - 19Cr - 3.0Mo - 5.1Cb (Nb) - 0.90Ti - 0.50Al - 18Fe Consumable Electrode or Vacuum Induction Melted 1775 °F (968 °C) Solution and Precipitation Heat Treated
  • 2009 SAE AMS5663M-2009 Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 52.5Ni - 19Cr - 3.0Mo - 5.1Cb (Nb) - 0.90Ti - 0.50Al - 18Fe Consumable Electrode or Vacuum Induction Melted 1775 °F (968 °C) Solution and Precipitation Heat Treated (Composition similar
  • 2004 SAE AMS5663M-2004 Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 52.5Ni 19Cr 3.0Mo 5.1Cb (Nb) 0.90Ti 0.50Al 19Fe Consumable Electrode or Vacuum Induction Melted 1775°F (968°C) Solution and Precipitation Heat Treated
  • 2003 SAE AMS5663L-2003 Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 52.5Ni - 19Cr - 3.0Mo - 5.1Cb - 0.90Ti - 0.50Al - 18Fe Consumable Electrode or Vacuum Induction Melted 1775 Degrees F (968 Degrees C) Solution and Precipitation Heat Treated UNS N0
  • 2002 SAE AMS5663K-2002 Nickel Alloy@ Corrosion and Heat-Resistant@ Bars@ Forgings@ and Rings 52.5Ni - 19Cr - 3.0Mo - 5.1Cb - 0.90Ti - 0.50Al - 18Fe Consumable Electrode or Vacuum Induction Melted 1775 °F (968 °C) Solution and Precipitation Heat Treated (UNS N07718)
  • 1997 SAE AMS5663J-1997 Nickel Alloy@ Corrosion and Heat Resistant@ Bars@ Forgings@ and Rings 52.5Ni - 19Cr - 3.0Mo - 5.1Cb - 0.90Ti - 0.50Al - 18Fe Consumable Electrode or Vacuum Induction Melted 1775 Degrees F (968 Degrees C) Solution and Precipitation Heat Treated (UNS N07718
  • 1996 SAE AMS5663H-1996 Nickel Alloy@ Corrosion & Heat Resistant@ Bars@ Forgings@ and Rings 52.5Ni - 19Cr - 3.0Mo - 5.1Cb - 0.90Ti - 0.50Al - 19Fe Consumable Electrode or Vacuum Induction Melted 1775 Degrees F (968 Degrees C) Solution and Precipitation Heat Treated (UNS N07718)
  • 1989 SAE AMS5663G-1989 ALLOY BARS, FORGINGS, AND RINGS, CORROSION AND HEAT RESISTANT 52.5Ni - 19Cr - 3.0Mo - 5.1(Cb + Ta) - 0.90Ti - 0.50Al - 19Fe Consumable Electrode or Vacuum Induction Melted 1775°F (968°C) Solution and Precipitation Heat Treated
  • 1989 SAE AMS5663F-1989 ALLOY BARS@ FORGINGS@ AND RINGS@ CORROSION AND HEAT RESISTANT 52.5Ni - 19Cr - 3.0Mo - 5.1(Cb + Ta) - 0.90Ti - 0.50Al - 19Fe Consumable Electrode or Vacuum Induction Melted 1750°F (955°C) Solution and Precipitation Heat Treated (UNS N07718)
  • 1987 SAE AMS5663E-1987 ALLOY BARS@ FORGINGS@ AND RINGS@ CORROSION AND HEAT RESISTANT 52.5Ni - 19Cr - 3.0Mo - 5.1(Cb + Ta) - 0.90Ti - 0.50Al - 19Fe Consumable Electrode or Vacuum Induction Melted 1750°F (955°C) Solution and Precipitation Heat Treated (UNS N07718)
  • 1980 SAE AMS5663D-1980 ALLOY BARS, FORGINGS, AND RINGS, CORROSION AND HEAT RESISTANT 52.5Ni - 19Cr - 3.0Mo - 5.1(Cb + Ta) - 0.90Ti - 0.50Al - 19Fe Consumable Electrode or Vacuum Induction Melted 1750°F (955°C) Solution and Precipitation Heat Treated
  • 1972 SAE AMS5663C-1972 ALLOY BARS, FORGINGS, AND RINGS, CORROSION AND HEAT RESISTANT Nickel Base - 19Cr - 3.1Mo - 5.1(Cb + Ta) - 0.90Ti - 0.50Al - 19Fe Consumable Electrode or Vacuum Induction Melted 1750 F (954.4 C) Solution and Precipitation Heat Treated
  • 1967 SAE AMS5663B-1967 ALLOY BARS, FORGINGS, AND RINGS, CORROSION AND HEAT RESISTANT Nickel Base - 19Cr - 3.1Mo - 5.1(Cb + Ta) - 0.90Ti - 0.50Al Consumable Electrode or Vacuum Induction Melted 1750 F (954.4 C) Solution and Precipitation Heat Treated
  • 1966 SAE AMS5663A-1966 ALLOY BARS, FORGINGS, AND RINGS, CORROSION AND HEAT RESISTANT Nickel Base - 19Cr - 3.1Mo - 5.1(Cb + Ta) - 0.90Ti - 0.50Al Solution and Precipitation Heat Treated Consumable Electrode or Vacuum Induction Melted
  • 1965 SAE AMS5663-1965 ALLOY BARS, FORGINGS, AND RINGS, CORROSION AND HEAT RESISTANT Nickel Base - 19Cr - 3.1Mo - 5.1(Cb + Ta) - 0.90Ti - 0.50Al Solution and Precipitation Heat Treated Consumable Electrode or Vacuum Induction Melted



Copyright ©2023 All Rights Reserved