SAE AMS5663P-2022
Nickel Alloy, Corrosion- and Heat-Resistant, Bars, Forgings, Rings, and Stock for Forgings and Rings, 52.5Ni - 19Cr - 3.0Mo - 5.1Cb (Nb) - 0.90Ti - 0.50Al - 18Fe, Consumable Electrode or Vacuum Induction Melted, 1775 °F (968 °C) Solution

Standard No.
SAE AMS5663P-2022
Release Date
1970
Published By
/
Latest
SAE AMS5663P-2022
Scope
This specification covers a corrosion- and heat-resistant nickel alloy in the form of bars, forgings, and flash welded rings in the solution and precipitation heat treated condition. Product covered by this specification is limited to 10.00 inches (254 mm) and under in nominal diameter or maximum cross-sectional dimension between parallel sides (thickness) and nominal cross sectional area of 78.54 in2 (503 cm2). Stock may be of any size for forging or flash welded rings.

SAE AMS5663P-2022 history

  • 1970 SAE AMS5663P-2022 Nickel Alloy, Corrosion- and Heat-Resistant, Bars, Forgings, Rings, and Stock for Forgings and Rings, 52.5Ni - 19Cr - 3.0Mo - 5.1Cb (Nb) - 0.90Ti - 0.50Al - 18Fe, Consumable Electrode or Vacuum Induction Melted, 1775 °F (968 °C) Solution
  • 2016 SAE AMS5663N-2016 Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 52.5Ni - 19Cr - 3.0Mo - 5.1Cb (Nb) - 0.90Ti - 0.50Al - 18Fe Consumable Electrode or Vacuum Induction Melted 1775 °F (968 °C) Solution and Precipitation Heat Treated
  • 2009 SAE AMS5663M-2009 Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 52.5Ni - 19Cr - 3.0Mo - 5.1Cb (Nb) - 0.90Ti - 0.50Al - 18Fe Consumable Electrode or Vacuum Induction Melted 1775 °F (968 °C) Solution and Precipitation Heat Treated (Composition similar
  • 2004 SAE AMS5663M-2004 Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 52.5Ni 19Cr 3.0Mo 5.1Cb (Nb) 0.90Ti 0.50Al 19Fe Consumable Electrode or Vacuum Induction Melted 1775°F (968°C) Solution and Precipitation Heat Treated
  • 2003 SAE AMS5663L-2003 Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 52.5Ni - 19Cr - 3.0Mo - 5.1Cb - 0.90Ti - 0.50Al - 18Fe Consumable Electrode or Vacuum Induction Melted 1775 Degrees F (968 Degrees C) Solution and Precipitation Heat Treated UNS N0
  • 2002 SAE AMS5663K-2002 Nickel Alloy@ Corrosion and Heat-Resistant@ Bars@ Forgings@ and Rings 52.5Ni - 19Cr - 3.0Mo - 5.1Cb - 0.90Ti - 0.50Al - 18Fe Consumable Electrode or Vacuum Induction Melted 1775 °F (968 °C) Solution and Precipitation Heat Treated (UNS N07718)
  • 1997 SAE AMS5663J-1997 Nickel Alloy@ Corrosion and Heat Resistant@ Bars@ Forgings@ and Rings 52.5Ni - 19Cr - 3.0Mo - 5.1Cb - 0.90Ti - 0.50Al - 18Fe Consumable Electrode or Vacuum Induction Melted 1775 Degrees F (968 Degrees C) Solution and Precipitation Heat Treated (UNS N07718
  • 1996 SAE AMS5663H-1996 Nickel Alloy@ Corrosion & Heat Resistant@ Bars@ Forgings@ and Rings 52.5Ni - 19Cr - 3.0Mo - 5.1Cb - 0.90Ti - 0.50Al - 19Fe Consumable Electrode or Vacuum Induction Melted 1775 Degrees F (968 Degrees C) Solution and Precipitation Heat Treated (UNS N07718)
  • 1989 SAE AMS5663G-1989 ALLOY BARS, FORGINGS, AND RINGS, CORROSION AND HEAT RESISTANT 52.5Ni - 19Cr - 3.0Mo - 5.1(Cb + Ta) - 0.90Ti - 0.50Al - 19Fe Consumable Electrode or Vacuum Induction Melted 1775°F (968°C) Solution and Precipitation Heat Treated
  • 1989 SAE AMS5663F-1989 ALLOY BARS@ FORGINGS@ AND RINGS@ CORROSION AND HEAT RESISTANT 52.5Ni - 19Cr - 3.0Mo - 5.1(Cb + Ta) - 0.90Ti - 0.50Al - 19Fe Consumable Electrode or Vacuum Induction Melted 1750°F (955°C) Solution and Precipitation Heat Treated (UNS N07718)
  • 1987 SAE AMS5663E-1987 ALLOY BARS@ FORGINGS@ AND RINGS@ CORROSION AND HEAT RESISTANT 52.5Ni - 19Cr - 3.0Mo - 5.1(Cb + Ta) - 0.90Ti - 0.50Al - 19Fe Consumable Electrode or Vacuum Induction Melted 1750°F (955°C) Solution and Precipitation Heat Treated (UNS N07718)
  • 1980 SAE AMS5663D-1980 ALLOY BARS, FORGINGS, AND RINGS, CORROSION AND HEAT RESISTANT 52.5Ni - 19Cr - 3.0Mo - 5.1(Cb + Ta) - 0.90Ti - 0.50Al - 19Fe Consumable Electrode or Vacuum Induction Melted 1750°F (955°C) Solution and Precipitation Heat Treated
  • 1972 SAE AMS5663C-1972 ALLOY BARS, FORGINGS, AND RINGS, CORROSION AND HEAT RESISTANT Nickel Base - 19Cr - 3.1Mo - 5.1(Cb + Ta) - 0.90Ti - 0.50Al - 19Fe Consumable Electrode or Vacuum Induction Melted 1750 F (954.4 C) Solution and Precipitation Heat Treated
  • 1967 SAE AMS5663B-1967 ALLOY BARS, FORGINGS, AND RINGS, CORROSION AND HEAT RESISTANT Nickel Base - 19Cr - 3.1Mo - 5.1(Cb + Ta) - 0.90Ti - 0.50Al Consumable Electrode or Vacuum Induction Melted 1750 F (954.4 C) Solution and Precipitation Heat Treated
  • 1966 SAE AMS5663A-1966 ALLOY BARS, FORGINGS, AND RINGS, CORROSION AND HEAT RESISTANT Nickel Base - 19Cr - 3.1Mo - 5.1(Cb + Ta) - 0.90Ti - 0.50Al Solution and Precipitation Heat Treated Consumable Electrode or Vacuum Induction Melted
  • 1965 SAE AMS5663-1965 ALLOY BARS, FORGINGS, AND RINGS, CORROSION AND HEAT RESISTANT Nickel Base - 19Cr - 3.1Mo - 5.1(Cb + Ta) - 0.90Ti - 0.50Al Solution and Precipitation Heat Treated Consumable Electrode or Vacuum Induction Melted
Nickel Alloy, Corrosion- and Heat-Resistant, Bars, Forgings, Rings, and Stock for Forgings and Rings, 52.5Ni - 19Cr - 3.0Mo - 5.1Cb (Nb) - 0.90Ti - 0.50Al - 18Fe, Consumable Electrode or Vacuum Induction Melted, 1775 °F (968 °C) Solution