Scope
This specification covers a corrosion and heat resistant cobalt alloy in the form of strip 0.100 inch (2.54 mm) and under in specified thickness and 4.000 inches (101.60 mm) and under in specified width.
SAE AMS5875B-2000 history
2018
SAE AMS5875D-2018
Cobalt Alloy@ Corrosion and Heat-Resistant@ Strip 20Cr - 15Ni - 40Co - 7.0Mo - 16Fe Solution Heat Treated@ Cold Rolled@ and Aged Vacuum Induction Plus Vacuum Consumable Electrode Melted (UNS R30003)
2012
SAE AMS5875C-2012
Cobalt Alloy, Corrosion and Heat-Resistant, Strip 20Cr - 15Ni - 40Co - 7.0Mo - 16Fe Solution Heat Treated, Cold Rolled, and Aged Vacuum Induction Plus Vacuum Consumable Electrode Melted
2011
SAE AMS5875A-2011
ALLOY STRIP, CORROSION AND HEAT RESISTANT 20Cr - 15Ni - 40Co - 7.0Mo - 16Fe Solution Heat Treated, Cold Rolled, and Aged
2002
SAE AMS5875C-2002
Cobalt Alloy, Corrosion and Heat-Resistant, Strip 20Cr - 15Ni - 40Co - 7.0Mo - 16Fe Solution Heat Treated, Cold Rolled, and Aged Vacuum Induction Plus Vacuum Consumable Electrode Melted UNS S30003
2000
SAE AMS5875B-2000
Cobalt Alloy, Corrosion and Heat Resistant, Strip 20Cr - 15Ni - 40Co - 7.0Mo - 16Fe Solution Heat Treated, Cold Rolled, and Aged
1993
SAE AMS5875B-1993
Cobalt Alloy@ Corrosion and Heat Resistant@ Strip 20Cr - 15Ni - 40Co - 7.0Mo - 16Fe Solution Heat Treated@ Cold Rolled@ and Aged (UNS R30003)
1984
SAE AMS5875-1984
ALLOY STRIP, CORROSION AND HEAT RESISTANT 40Co - 20Cr - 15Ni - 7.0Mo - 0.06Be - 16Fe Vacuum Induction Plus Vacuum Consumable Electrode Melted Solution Heat Treated, Cold Rolled, and Aged
Copyright ©2024 All Rights Reserved