SAE AMS5875-1984
ALLOY STRIP, CORROSION AND HEAT RESISTANT 40Co - 20Cr - 15Ni - 7.0Mo - 0.06Be - 16Fe Vacuum Induction Plus Vacuum Consumable Electrode Melted Solution Heat Treated, Cold Rolled, and Aged

Standard No.
SAE AMS5875-1984
Release Date
1984
Published By
Society of Automotive Engineers (SAE)
Status
 2000-08
Replace By
SAE AMS5875B-1993
Latest
SAE AMS5875D-2018
Scope
This specification covers a high-strength, corrosion and heat resistant cobalt alloy in the form of strip up to 0.100 in. (2.50 mm), incl, in specified thickness and up to 4.000 in. (100.00 mm) in specified width.

SAE AMS5875-1984 history

  • 2018 SAE AMS5875D-2018 Cobalt Alloy@ Corrosion and Heat-Resistant@ Strip 20Cr - 15Ni - 40Co - 7.0Mo - 16Fe Solution Heat Treated@ Cold Rolled@ and Aged Vacuum Induction Plus Vacuum Consumable Electrode Melted (UNS R30003)
  • 2012 SAE AMS5875C-2012 Cobalt Alloy, Corrosion and Heat-Resistant, Strip 20Cr - 15Ni - 40Co - 7.0Mo - 16Fe Solution Heat Treated, Cold Rolled, and Aged Vacuum Induction Plus Vacuum Consumable Electrode Melted
  • 2011 SAE AMS5875A-2011 ALLOY STRIP, CORROSION AND HEAT RESISTANT 20Cr - 15Ni - 40Co - 7.0Mo - 16Fe Solution Heat Treated, Cold Rolled, and Aged
  • 2002 SAE AMS5875C-2002 Cobalt Alloy, Corrosion and Heat-Resistant, Strip 20Cr - 15Ni - 40Co - 7.0Mo - 16Fe Solution Heat Treated, Cold Rolled, and Aged Vacuum Induction Plus Vacuum Consumable Electrode Melted UNS S30003
  • 2000 SAE AMS5875B-2000 Cobalt Alloy, Corrosion and Heat Resistant, Strip 20Cr - 15Ni - 40Co - 7.0Mo - 16Fe Solution Heat Treated, Cold Rolled, and Aged
  • 1993 SAE AMS5875B-1993 Cobalt Alloy@ Corrosion and Heat Resistant@ Strip 20Cr - 15Ni - 40Co - 7.0Mo - 16Fe Solution Heat Treated@ Cold Rolled@ and Aged (UNS R30003)
  • 1984 SAE AMS5875-1984 ALLOY STRIP, CORROSION AND HEAT RESISTANT 40Co - 20Cr - 15Ni - 7.0Mo - 0.06Be - 16Fe Vacuum Induction Plus Vacuum Consumable Electrode Melted Solution Heat Treated, Cold Rolled, and Aged