SAE AMS5875C-2012
Cobalt Alloy, Corrosion and Heat-Resistant, Strip 20Cr - 15Ni - 40Co - 7.0Mo - 16Fe Solution Heat Treated, Cold Rolled, and Aged Vacuum Induction Plus Vacuum Consumable Electrode Melted
Home
SAE AMS5875C-2012
Standard No.
SAE AMS5875C-2012
Release Date
2012
Published By
Society of Automotive Engineers (SAE)
Status
Be replaced
2018-08
Replace By
SAE AMS5875D-2018
Latest
SAE AMS5875D-2018
Scope
This specification covers a corrosion and heat-resistant cobalt alloy in the form of strip 0.100 inch (2.54 mm) and under in specified thickness and 4.000inches (101.60 mm) and under in specified width.
SAE AMS5875C-2012 history
2018
SAE AMS5875D-2018
Cobalt Alloy@ Corrosion and Heat-Resistant@ Strip 20Cr - 15Ni - 40Co - 7.0Mo - 16Fe Solution Heat Treated@ Cold Rolled@ and Aged Vacuum Induction Plus Vacuum Consumable Electrode Melted (UNS R30003)
2012
SAE AMS5875C-2012
Cobalt Alloy, Corrosion and Heat-Resistant, Strip 20Cr - 15Ni - 40Co - 7.0Mo - 16Fe Solution Heat Treated, Cold Rolled, and Aged Vacuum Induction Plus Vacuum Consumable Electrode Melted
2011
SAE AMS5875A-2011
ALLOY STRIP, CORROSION AND HEAT RESISTANT 20Cr - 15Ni - 40Co - 7.0Mo - 16Fe Solution Heat Treated, Cold Rolled, and Aged
2002
SAE AMS5875C-2002
Cobalt Alloy, Corrosion and Heat-Resistant, Strip 20Cr - 15Ni - 40Co - 7.0Mo - 16Fe Solution Heat Treated, Cold Rolled, and Aged Vacuum Induction Plus Vacuum Consumable Electrode Melted UNS S30003
2000
SAE AMS5875B-2000
Cobalt Alloy, Corrosion and Heat Resistant, Strip 20Cr - 15Ni - 40Co - 7.0Mo - 16Fe Solution Heat Treated, Cold Rolled, and Aged
1993
SAE AMS5875B-1993
Cobalt Alloy@ Corrosion and Heat Resistant@ Strip 20Cr - 15Ni - 40Co - 7.0Mo - 16Fe Solution Heat Treated@ Cold Rolled@ and Aged (UNS R30003)
1984
SAE AMS5875-1984
ALLOY STRIP, CORROSION AND HEAT RESISTANT 40Co - 20Cr - 15Ni - 7.0Mo - 0.06Be - 16Fe Vacuum Induction Plus Vacuum Consumable Electrode Melted Solution Heat Treated, Cold Rolled, and Aged
Copyright ©2024 All Rights Reserved