SAE AMS5664A-1967
ALLOY BARS, FORGINGS, AND RINGS, CORROSION AND HEAT RESISTANT Nickel Base - 19Cr - 3.1Mo - 5.1(Cb + Ta) - 0.90Ti - 0.50Al Consumable Electrode or Vacuum Induction Melted 1950 F (1065.6 C) Solution Treated
Home
SAE AMS5664A-1967
Standard No.
SAE AMS5664A-1967
Release Date
1967
Published By
Society of Automotive Engineers (SAE)
Status
Be replaced
Replace By
SAE AMS5664B-1980
Latest
SAE AMS5664G-2022
SAE AMS5664A-1967 history
1970
SAE AMS5664G-2022
2017
SAE AMS5664F-2017
Nickel Alloy@ Corrosion and Heat Resistant@ Bars@ Forgings@ and Rings 52.5Ni - 19Cr - 3.0Mo - 5.1Cb (Nb) - 0.90Ti - 0.50Al - 18Fe Consumable Electrode or Vacuum Induction Melted 1950 °F (1066 °C) Solution Heat Treated@ Precipitation Hardenable (UNS N07718
2006
SAE AMS5664E-2006
Nickel Alloy, Corrosion and Heat Resistant, Bars, Forgings, and Rings 52.5Ni - 19Cr - 3.0Mo - 5.1Cb - 0.90Ti - 0.50Al - 18Fe Consumable Electrode or Vacuum Induction Melted 1950 °F (1066 °C) Solution Heat Treated, Precipitation Hardenable
2001
SAE AMS5664E-2001
Nickel Alloy, Corrosion and Heat Resistant, Bars, Forgings, and Rings 52.5Ni - 19Cr - 3.0Mo - 5.1Cb - 0.90Ti - 0.50A1 - 18Fe Consumable Electrode or Vacuum Induction Melted 1950 Degrees F (1066 Degrees C) Solution Heat Treated, Precipitation Hardenable U
2001
SAE AMS5664B-2001
Nickel Alloy@ Corrosion and Heat Resistant@ Bars@ Forgings@ and Rings 52.5Ni - 19Cr - 3.0Mo - 5.1Cb - 0.90Ti - 0.50A1 - 18Fe Consumable Electrode or Vacuum Induction Melted 1950 Degrees F (1066 Degrees C) Solution Heat Treated@ Precipitation Hardenable (U
1994
SAE AMS5664D-1994
Nickel Alloy@ Corrosion and Heat Resistant@ Bars@ Forgings@ and Rings 52.5Ni - 19Cr - 3.0Mo - 5.1Cb - 0.90Ti - 0.50A1 - 18Fe Consumable Electrode or Vacuum Induction Melted 1950 Degrees F (1066 Degrees C) Solution Heat Treated@ Precipitation Hardenable (U
1990
SAE AMS5664C-1990
ALLOY BARS@ FORGINGS@ AND RINGS@ CORROSION AND HEAT RESISTANT 52.5Ni - 19Cr - 3.0Mo - 5.1(Cb+Ta) - 0.90Ti - 0.50Al - 19Fe Consumable Electrode or Vacuum Induction Melted 1950°F (1066°C) Solution Heat Treated@ Precipitation Hardenable (UNS N07718)
1980
SAE AMS5664B-1980
ALLOY BARS, FORGINGS, AND RINGS, CORROSION AND HEAT RESISTANT 52.5Ni - 19Cr - 3.0Mo - 5.1(Cb+Ta) - 0.90Ti - 0.50Al - 19Fe Consumable Electrode or Vacuum Induction Melted 1950° F (1065° C) Solution Treated
1967
SAE AMS5664A-1967
ALLOY BARS, FORGINGS, AND RINGS, CORROSION AND HEAT RESISTANT Nickel Base - 19Cr - 3.1Mo - 5.1(Cb + Ta) - 0.90Ti - 0.50Al Consumable Electrode or Vacuum Induction Melted 1950 F (1065.6 C) Solution Treated
1965
SAE AMS5664-1965
ALLOY BARS, FORGINGS, AND RINGS, CORROSION AND HEAT RESISTANT Nickel Base - 19Cr - 3.1Mo - 5.1(Cb + Ta) - 0.90Ti - 0.50Al Consumable Electrode Melted, Solution Treated at 1950 F (1065.6 C)
Copyright ©2023 All Rights Reserved