SAE AMS5664G-2022
Nickel Alloy, Corrosion- and Heat-Resistant, Bars, Forgings, Extrusions, Rings, and Stock for Forgings and Rings 52.5Ni - 19Cr - 3.0Mo - 5.1Cb (Nb) - 0.90Ti - 0.50Al - 18Fe Consumable Electrode or Vacuum Induction Melted 1950 °F (1066 °C)

Standard No.
SAE AMS5664G-2022
Release Date
1970
Published By
/
Latest
SAE AMS5664G-2022
Scope
This specification covers a corrosion- and heat-resistant nickel alloy in the form of bars, forgings, flash welded rings in the solution heat treated condition, Product covered by this specification is limited to 10.00 inches (254 mm) and under in nominal diameter or maximum cross-sectional dimension between parallel sides (thickness) and 78.54 square inches (503 cm2) in cross-sectional area. Stock may be of any size for forging or flash welded rings.

SAE AMS5664G-2022 history

  • 1970 SAE AMS5664G-2022 Nickel Alloy, Corrosion- and Heat-Resistant, Bars, Forgings, Extrusions, Rings, and Stock for Forgings and Rings 52.5Ni - 19Cr - 3.0Mo - 5.1Cb (Nb) - 0.90Ti - 0.50Al - 18Fe Consumable Electrode or Vacuum Induction Melted 1950 °F (1066 °C)
  • 2017 SAE AMS5664F-2017 Nickel Alloy@ Corrosion and Heat Resistant@ Bars@ Forgings@ and Rings 52.5Ni - 19Cr - 3.0Mo - 5.1Cb (Nb) - 0.90Ti - 0.50Al - 18Fe Consumable Electrode or Vacuum Induction Melted 1950 °F (1066 °C) Solution Heat Treated@ Precipitation Hardenable (UNS N07718
  • 2006 SAE AMS5664E-2006 Nickel Alloy, Corrosion and Heat Resistant, Bars, Forgings, and Rings 52.5Ni - 19Cr - 3.0Mo - 5.1Cb - 0.90Ti - 0.50Al - 18Fe Consumable Electrode or Vacuum Induction Melted 1950 °F (1066 °C) Solution Heat Treated, Precipitation Hardenable
  • 2001 SAE AMS5664E-2001 Nickel Alloy, Corrosion and Heat Resistant, Bars, Forgings, and Rings 52.5Ni - 19Cr - 3.0Mo - 5.1Cb - 0.90Ti - 0.50A1 - 18Fe Consumable Electrode or Vacuum Induction Melted 1950 Degrees F (1066 Degrees C) Solution Heat Treated, Precipitation Hardenable U
  • 2001 SAE AMS5664B-2001 Nickel Alloy@ Corrosion and Heat Resistant@ Bars@ Forgings@ and Rings 52.5Ni - 19Cr - 3.0Mo - 5.1Cb - 0.90Ti - 0.50A1 - 18Fe Consumable Electrode or Vacuum Induction Melted 1950 Degrees F (1066 Degrees C) Solution Heat Treated@ Precipitation Hardenable (U
  • 1994 SAE AMS5664D-1994 Nickel Alloy@ Corrosion and Heat Resistant@ Bars@ Forgings@ and Rings 52.5Ni - 19Cr - 3.0Mo - 5.1Cb - 0.90Ti - 0.50A1 - 18Fe Consumable Electrode or Vacuum Induction Melted 1950 Degrees F (1066 Degrees C) Solution Heat Treated@ Precipitation Hardenable (U
  • 1990 SAE AMS5664C-1990 ALLOY BARS@ FORGINGS@ AND RINGS@ CORROSION AND HEAT RESISTANT 52.5Ni - 19Cr - 3.0Mo - 5.1(Cb+Ta) - 0.90Ti - 0.50Al - 19Fe Consumable Electrode or Vacuum Induction Melted 1950°F (1066°C) Solution Heat Treated@ Precipitation Hardenable (UNS N07718)
  • 1980 SAE AMS5664B-1980 ALLOY BARS, FORGINGS, AND RINGS, CORROSION AND HEAT RESISTANT 52.5Ni - 19Cr - 3.0Mo - 5.1(Cb+Ta) - 0.90Ti - 0.50Al - 19Fe Consumable Electrode or Vacuum Induction Melted 1950° F (1065° C) Solution Treated
  • 1967 SAE AMS5664A-1967 ALLOY BARS, FORGINGS, AND RINGS, CORROSION AND HEAT RESISTANT Nickel Base - 19Cr - 3.1Mo - 5.1(Cb + Ta) - 0.90Ti - 0.50Al Consumable Electrode or Vacuum Induction Melted 1950 F (1065.6 C) Solution Treated
  • 1965 SAE AMS5664-1965 ALLOY BARS, FORGINGS, AND RINGS, CORROSION AND HEAT RESISTANT Nickel Base - 19Cr - 3.1Mo - 5.1(Cb + Ta) - 0.90Ti - 0.50Al Consumable Electrode Melted, Solution Treated at 1950 F (1065.6 C)
Nickel Alloy, Corrosion- and Heat-Resistant, Bars, Forgings, Extrusions, Rings, and Stock for Forgings and Rings 52.5Ni - 19Cr - 3.0Mo - 5.1Cb (Nb) - 0.90Ti - 0.50Al - 18Fe Consumable Electrode or Vacuum Induction Melted 1950 °F (1066 °C)



Copyright ©2024 All Rights Reserved