Scope
This specification covers an aluminum bronze alloy in the form of centrifugal and continuous castings. These castings have been used typically for bearings requiring abrasion resistance, good ductility, and good retention of hardness at moderate temperatures, but usage is not limited to such applications.

SAE AMS4880D-2005 Referenced Document

  • ASTM E1417-05 Standard Practice for Liquid Penetrant Testing*2024-04-18 Update
  • ASTM E1742-05 Standard Practice for Radiographic Examination*2024-04-18 Update
  • ASTM E478-03 Standard Test Methods for Chemical Analysis of Copper Alloys*2024-04-18 Update
  • ASTM E8-04 Standard Test Methods for Tension Testing of Metallic Materials*2024-04-18 Update
  • ASTM E8M-04 Standard Test Methods for Tension Testing of Metallic Materials [Metric] *2024-04-18 Update
  • SAE AMS2360C-2001 Room Temperature Tensile Properties of Castings
  • SAE AMS2694A-1984 Repair Welding of Aerospace Castings
  • SAE AMS2750C-1990 Pyrometry (Reaffirmed: 01 Apr 1994)
  • SAE AMS2804C-2001 Identification Castings

SAE AMS4880D-2005 history

  • 2018 SAE AMS4880D-2018 Aluminum Bronze Alloy, Centrifugal and Continuous-Cast Castings 81.5Cu - 10.3Al - 5.0Ni - 2.8Fe Quench Hardened and Temper Annealed (TQ50)
  • 2005 SAE AMS4880D-2005 Aluminum Bronze Alloy, Centrifugal and Continuous-Cast Castings 81.5Cu - 10.3Al - 5.0Ni - 2.8Fe Quench Hardened and Temper Annealed (TQ50) UNS C95510
  • 1995 SAE AMS4880C-1995 Aluminum Bronze Alloy, Centrifugal and Continuous-Cast Castings 81.5Cu - 10.3Al - 5.0Ni - 2.8Fe Quench Hardened and Temper Annealed (UNS C95510)
  • 1989 SAE AMS4880B-1989 ALUMINUM BRONZE CASTINGS@ CENTRIFUGAL AND CONTINUOUS CAST 81.5Cu - 10.3Al - 5.0Ni - 2.8Fe Solution Heat Treated and Tempered (UNS C95510)
  • 1989 SAE AMS4880A-1989 ALUMINUM BRONZE CASTINGS, CENTRIFUGAL 81.5Cu - 10.3Al - 5.0Ni - 2.8Fe Solution Heat Treated and Tempered
  • 1984 SAE AMS4880A-1984 ALUMINUM BRONZE CASTINGS@ CENTRIFUGAL 81.5Cu - 10.3Al - 5.0Ni - 2.8Fe Solution Heat Treated and tempered
  • 1952 SAE AMS4880-1952 ALUMINUM BRONZE CASTINGS@ CENTRIFUGAL 81.5Cu - 10.3Al - 5Ni - 2.8Fe Heat Treated



Copyright ©2024 All Rights Reserved