SAE AMS4880A-1984
ALUMINUM BRONZE CASTINGS@ CENTRIFUGAL 81.5Cu - 10.3Al - 5.0Ni - 2.8Fe Solution Heat Treated and tempered

Standard No.
SAE AMS4880A-1984
Release Date
1984
Published By
SAE - SAE International
Status
Replace By
SAE AMS4880A-1989
Latest
SAE AMS4880D-2018
Scope
Form: This specification covers one type of aluminum bronze in the form of centrifugal castings. Application: Primarily for bearings requiring abrasion resistance@ good ductility@ and good retention of hardness at moderate temperatures.

SAE AMS4880A-1984 history

  • 2018 SAE AMS4880D-2018 Aluminum Bronze Alloy, Centrifugal and Continuous-Cast Castings 81.5Cu - 10.3Al - 5.0Ni - 2.8Fe Quench Hardened and Temper Annealed (TQ50)
  • 2005 SAE AMS4880D-2005 Aluminum Bronze Alloy, Centrifugal and Continuous-Cast Castings 81.5Cu - 10.3Al - 5.0Ni - 2.8Fe Quench Hardened and Temper Annealed (TQ50) UNS C95510
  • 1995 SAE AMS4880C-1995 Aluminum Bronze Alloy, Centrifugal and Continuous-Cast Castings 81.5Cu - 10.3Al - 5.0Ni - 2.8Fe Quench Hardened and Temper Annealed (UNS C95510)
  • 1989 SAE AMS4880B-1989 ALUMINUM BRONZE CASTINGS@ CENTRIFUGAL AND CONTINUOUS CAST 81.5Cu - 10.3Al - 5.0Ni - 2.8Fe Solution Heat Treated and Tempered (UNS C95510)
  • 1989 SAE AMS4880A-1989 ALUMINUM BRONZE CASTINGS, CENTRIFUGAL 81.5Cu - 10.3Al - 5.0Ni - 2.8Fe Solution Heat Treated and Tempered
  • 1984 SAE AMS4880A-1984 ALUMINUM BRONZE CASTINGS@ CENTRIFUGAL 81.5Cu - 10.3Al - 5.0Ni - 2.8Fe Solution Heat Treated and tempered
  • 1952 SAE AMS4880-1952 ALUMINUM BRONZE CASTINGS@ CENTRIFUGAL 81.5Cu - 10.3Al - 5Ni - 2.8Fe Heat Treated