Scope
This specification covers a cobalt alloy in the form of powder. This product has been used typically for producing plasma spray coatings to provide surfaces resistant to wear, corrosion, and abrasion, but usage is not limited to such applications.

SAE AMS5791C-2009 Referenced Document

  • ASTM B214-07 Standard Test Method for Sieve Analysis of Metal Powders*2024-04-19 Update
  • ASTM B215-08 Standard Practices for Sampling Metal Powders*2024-04-19 Update

SAE AMS5791C-2009 history

  • 2021 SAE AMS5791D-2021 Cobalt Alloy, Powder, Plasma Spray 56.5Co - 25.5Cr - 10.5Ni - 7.5W
  • 2015 SAE AMS5791C-2015 Cobalt Alloy, Powder, Plasma Spray 56.5Co - 25.5Cr - 10.5Ni - 7.5W
  • 2011 SAE AMS5791-2011 POWDER, PLASMA SPRAY 56.5Co - 25.5Cr - 10.5Ni - 7.5W
  • 2009 SAE AMS5791C-2009 Cobalt Alloy, Powder, Plasma Spray 56.5Co 25.5Cr 10.5Ni 7.5W
  • 2004 SAE AMS5791B-2004 Cobalt Alloy, Powder, Plasma Spray 56.5Co 25.5Cr 10.5Ni 7.5W
  • 1998 SAE AMS5791A-1998 Cobalt Alloy, Powder, Plasma Spray 56.5Co - 25.5Cr - 10.5Ni - 7.5W
  • 1992 SAE AMS5791A-1992 Cobalt Alloy@ Powder@ Plasma Spray 56.5Co - 25.5Cr - 10.5Ni - 7.5W



Copyright ©2024 All Rights Reserved