SAE AMS5791B-2004
Cobalt Alloy, Powder, Plasma Spray 56.5Co 25.5Cr 10.5Ni 7.5W
Home
SAE AMS5791B-2004
Standard No.
SAE AMS5791B-2004
Release Date
2004
Published By
Society of Automotive Engineers (SAE)
Status
Withdraw
Replace By
SAE AMS5791C-2009
Latest
SAE AMS5791D-2021
Scope
This specification covers a cobalt alloy in the form of powder. This product has been used typically for producing plasma spray coatings to provide surfaces resistant to wear, corrosion, and abrasion, but usage is not limited to such applications.
SAE AMS5791B-2004 history
2021
SAE AMS5791D-2021
Cobalt Alloy, Powder, Plasma Spray 56.5Co - 25.5Cr - 10.5Ni - 7.5W
2015
SAE AMS5791C-2015
Cobalt Alloy, Powder, Plasma Spray 56.5Co - 25.5Cr - 10.5Ni - 7.5W
2011
SAE AMS5791-2011
POWDER, PLASMA SPRAY 56.5Co - 25.5Cr - 10.5Ni - 7.5W
2009
SAE AMS5791C-2009
Cobalt Alloy, Powder, Plasma Spray 56.5Co 25.5Cr 10.5Ni 7.5W
2004
SAE AMS5791B-2004
Cobalt Alloy, Powder, Plasma Spray 56.5Co 25.5Cr 10.5Ni 7.5W
1998
SAE AMS5791A-1998
Cobalt Alloy, Powder, Plasma Spray 56.5Co - 25.5Cr - 10.5Ni - 7.5W
1992
SAE AMS5791A-1992
Cobalt Alloy@ Powder@ Plasma Spray 56.5Co - 25.5Cr - 10.5Ni - 7.5W