SAE AMS5709H-2008
Nickel Alloy, Corrosion and Heat-Resistant, Bars and Forgings 58Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al - 0.05Zr - 0.006B Consumable Electrode or Vacuum Induction Melted 1975 °F (1079 °C) Solution, Stabilization, and Precipitation Heat Treated UNS N

Standard No.
SAE AMS5709H-2008
Release Date
2008
Published By
Society of Automotive Engineers (SAE)
Status
Replace By
SAE AMS5709H-2013
Latest
SAE AMS5709J-2019
Scope
This specification covers a corrosion and heat resistant nickel alloy in the form of bars, forgings, and forging stock. These products have been used typically for parts, such as pins, nuts, and turbine blades, requiring high strength up to 1500 ?F (816 ?C) and oxidation resistance up to 1750 ?F (954 ?C), but usage is not limited to such applications.

SAE AMS5709H-2008 Referenced Document

  • ASTM E139-06 Standard Test Methods for Conducting Creep, Creep-Rupture, and Stress-Rupture Tests of Metallic Materials*2024-04-18 Update
  • ASTM E18-08 Standard Test Methods for Rockwell Hardness of Metallic Materials*2024-04-18 Update
  • SAE AMS2261 TOLERANCES Nickel and Nickel Base Alloy Bars
  • SAE AMS2261H-2007 Tolerances, Nickel, Nickel Alloy, and Cobalt Alloy, Bars, Rods, and Wire
  • SAE AMS2269F-2006 Chemical Check Analysis Limits Nickel, Nickel Alloys, and Cobalt Alloys [Superseded: SAE AMS 2268B]
  • SAE AMS2371H-2007 Quality Assurance Sampling and Testing Corrosion and Heat-Resistant Steels and Alloys Wrought Products and Forging Stock*2024-04-18 Update
  • SAE AMS2374D-2002 Quality Assurance Sampling and Testing Corrosion and Heat-Resistant Steel and Alloy Forgings
  • SAE AMS2750D-2005 (R) Pyrometry
  • SAE AMS2806C-2008 Identification Bars, Wire, Mechanical Tubing, and Extrusions Carbon and Alloy Steels and Corrosion and Heat-Resistant Steels and Alloys
  • SAE AMS2808D-2001 Identification Forgings [Superseded: SAE AMS-STD-184A, SAE AMS-STD-184]

SAE AMS5709H-2008 history

  • 2019 SAE AMS5709J-2019 Nickel Alloy, Corrosion and Heat-Resistant, Bars and Forgings 58Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al - 0.05Zr - 0.006B Consumable Electrode or Vacuum Induction Melted 1975 °F (1079 °C) Solution, Stabilization, and Precipitation Heat Treated
  • 2013 SAE AMS5709H-2013 Nickel Alloy, Corrosion and Heat-Resistant, Bars and Forgings 58Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al - 0.05Zr - 0.006B Consumable Electrode or Vacuum Induction Melted 1975 °F (1079 °C) Solution, Stabilization, and Precipitation Heat Treated
  • 2008 SAE AMS5709H-2008 Nickel Alloy, Corrosion and Heat-Resistant, Bars and Forgings 58Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al - 0.05Zr - 0.006B Consumable Electrode or Vacuum Induction Melted 1975 °F (1079 °C) Solution, Stabilization, and Precipitation Heat Treated UNS N
  • 2006 SAE AMS5709G-2006 Nickel Alloy, Corrosion and Heat Resistant, Bars and Forgings 58Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al - 0.05Zr - 0.006B Consumable Electrode or Vacuum Induction Melted 1975 °F (1079 °C) Solution, Stabilization, and Precipitation Heat Treated
  • 2000 SAE AMS5709G-2000 Nickel Alloy, Corrosion and Heat Resistant, Bars and Forgings 58Ni 19.5Cr 13.5Co 4.3Mo 3.0Ti 1.4Al 0.05Zr 0.006B, Consumable Electrode or Vacuum Induction Melted, 1975°F (1079°C) Solution, Stabilization, and Precipitation Heat Treated
  • 1994 SAE AMS5709F-1994 Nickel Alloy@ Corrosion and Heat Resistant@ Bars and Forgings 58Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al - 0.05Zr - 0.006B Consumable Electrode or Vacuum Induction Melted 1975 Degrees F (1079 Degrees C) Solution@ Stabilization@ and Precipitation Heat
  • 1988 SAE AMS5709E-1988 ALLOY BARS AND FORGINGS@ CORROSION AND HEAT RESISTANT 58Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4A1 - 0.05Zr - 0.006B Consumable Electrode or Vacuum Induction Melted 1975 Degrees F (1079 Degrees C) Solution@ Stabilization@ and Precipitation Heat Treated
  • 1981 SAE AMS5709D-1981 ALLOY BARS AND FORGINGS, CORROSION AND HEAT RESISTANT 58Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al Consumable Electrode or Vacuum Induction Melted 1975°F (1080°C) Solution, Stabilization, and Precipitation Heat Treated
  • 1974 SAE AMS5709C-1974 ALLOY BARS AND FORGINGS, CORROSION AND HEAT RESISTANT Nickel Base - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al Consumable Electrode or Vacuum Induction Melted 1975° F (1079.4° C) Solution, Stabilization, and Precipitation Heat Treated
  • 1973 SAE AMS5709B-1973 ALLOY BARS AND FORGINGS, CORROSION AND HEAT RESISTANT Nickel Base - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al Consumable Electrode or Vacuum Induction Melted 1975° F (1079.4° C) Solution, Stabilization, and Precipitation Heat Treated
  • 1970 SAE AMS5709A-1970 ALLOY BARS AND FORGINGS, CORROSION AND HEAT RESISTANT Nickel Base - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al Consumable Electrode or Vacuum Induction Melted 1975 F (1079.4 C) Solution, Stabilization, and Precipitation Heat Treated
  • 1963 SAE AMS5709-1963 ALLOY BARS AND FORGINGS, CORROSION AND HEAT RESISTANT Nickel Base - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al Solution, Stabilization, and Precipitation Heat Treated. 1975 F (1079.4 C) Treatment Consumable Electrode or Vacuum Induction Melted



Copyright ©2024 All Rights Reserved