SAE AMS5709G-2006
Nickel Alloy, Corrosion and Heat Resistant, Bars and Forgings 58Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al - 0.05Zr - 0.006B Consumable Electrode or Vacuum Induction Melted 1975 °F (1079 °C) Solution, Stabilization, and Precipitation Heat Treated

Standard No.
SAE AMS5709G-2006
Release Date
2006
Published By
Society of Automotive Engineers (SAE)
Status
Replace By
SAE AMS5709H-2008
Latest
SAE AMS5709J-2019
Scope
This specification covers a corrosion and heat resistant nickel alloy in the form of bars, forgings, and forging stock.

SAE AMS5709G-2006 history

  • 2019 SAE AMS5709J-2019 Nickel Alloy, Corrosion and Heat-Resistant, Bars and Forgings 58Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al - 0.05Zr - 0.006B Consumable Electrode or Vacuum Induction Melted 1975 °F (1079 °C) Solution, Stabilization, and Precipitation Heat Treated
  • 2013 SAE AMS5709H-2013 Nickel Alloy, Corrosion and Heat-Resistant, Bars and Forgings 58Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al - 0.05Zr - 0.006B Consumable Electrode or Vacuum Induction Melted 1975 °F (1079 °C) Solution, Stabilization, and Precipitation Heat Treated
  • 2008 SAE AMS5709H-2008 Nickel Alloy, Corrosion and Heat-Resistant, Bars and Forgings 58Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al - 0.05Zr - 0.006B Consumable Electrode or Vacuum Induction Melted 1975 °F (1079 °C) Solution, Stabilization, and Precipitation Heat Treated UNS N
  • 2006 SAE AMS5709G-2006 Nickel Alloy, Corrosion and Heat Resistant, Bars and Forgings 58Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al - 0.05Zr - 0.006B Consumable Electrode or Vacuum Induction Melted 1975 °F (1079 °C) Solution, Stabilization, and Precipitation Heat Treated
  • 2000 SAE AMS5709G-2000 Nickel Alloy, Corrosion and Heat Resistant, Bars and Forgings 58Ni 19.5Cr 13.5Co 4.3Mo 3.0Ti 1.4Al 0.05Zr 0.006B, Consumable Electrode or Vacuum Induction Melted, 1975°F (1079°C) Solution, Stabilization, and Precipitation Heat Treated
  • 1994 SAE AMS5709F-1994 Nickel Alloy@ Corrosion and Heat Resistant@ Bars and Forgings 58Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al - 0.05Zr - 0.006B Consumable Electrode or Vacuum Induction Melted 1975 Degrees F (1079 Degrees C) Solution@ Stabilization@ and Precipitation Heat
  • 1988 SAE AMS5709E-1988 ALLOY BARS AND FORGINGS@ CORROSION AND HEAT RESISTANT 58Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4A1 - 0.05Zr - 0.006B Consumable Electrode or Vacuum Induction Melted 1975 Degrees F (1079 Degrees C) Solution@ Stabilization@ and Precipitation Heat Treated
  • 1981 SAE AMS5709D-1981 ALLOY BARS AND FORGINGS, CORROSION AND HEAT RESISTANT 58Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al Consumable Electrode or Vacuum Induction Melted 1975°F (1080°C) Solution, Stabilization, and Precipitation Heat Treated
  • 1974 SAE AMS5709C-1974 ALLOY BARS AND FORGINGS, CORROSION AND HEAT RESISTANT Nickel Base - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al Consumable Electrode or Vacuum Induction Melted 1975° F (1079.4° C) Solution, Stabilization, and Precipitation Heat Treated
  • 1973 SAE AMS5709B-1973 ALLOY BARS AND FORGINGS, CORROSION AND HEAT RESISTANT Nickel Base - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al Consumable Electrode or Vacuum Induction Melted 1975° F (1079.4° C) Solution, Stabilization, and Precipitation Heat Treated
  • 1970 SAE AMS5709A-1970 ALLOY BARS AND FORGINGS, CORROSION AND HEAT RESISTANT Nickel Base - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al Consumable Electrode or Vacuum Induction Melted 1975 F (1079.4 C) Solution, Stabilization, and Precipitation Heat Treated
  • 1963 SAE AMS5709-1963 ALLOY BARS AND FORGINGS, CORROSION AND HEAT RESISTANT Nickel Base - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al Solution, Stabilization, and Precipitation Heat Treated. 1975 F (1079.4 C) Treatment Consumable Electrode or Vacuum Induction Melted