SAE AMS5707K-2007
Nickel Alloy, Corrosion and Heat Resistant, Bars, Forgings and Rings 58Ni 19.5Cr 13.5Co 4.3Mo 3.0Ti 1.4Al 0.05Zr 0.006B Consumable Electrode or Vacuum Induction Melted 1825 to 1900°F (996 to 1038°C) Solution, Stabilization, and Precipitation Heat Treated

Standard No.
SAE AMS5707K-2007
Release Date
2007
Published By
Society of Automotive Engineers (SAE)
Status
Replace By
SAE AMS5707L-2008
Latest
SAE AMS5707P-2023
Scope
This specification covers a corrosion and heat resistant nickel alloy in the form of bars, forgings, flash welded rings, and stock for forging or flash welded rings. These products have been used typically for parts, such as cases, requiring high strength up to 1500 °F (816 °C) and oxidation resistance up 1750 °F (954 °C), but usage is not limited to such applications.

SAE AMS5707K-2007 history

  • 1970 SAE AMS5707P-2023 Nickel Alloy, Corrosion- and Heat-Resistant, Bars, Forgings, Rings, and Forging Stock 57Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al - 0.05Zr - 0.006B Consumable Electrode Remelted or Vacuum Induction Melted 1825 to 1900 °F (996 to 1038 °C)
  • 2017 SAE AMS5707N-2017 Nickel Alloy@ Corrosion and Heat-Resistant@ Bars@ Forgings@ and Rings 57Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al - 0.05Zr - 0.006B Consumable Electrode Remelted or Vacuum Induction Melted 1825 to 1900 °F (996 to 1038 °C) Solution@ Stabilization@ and P
  • 2015 SAE AMS5707M-2015 Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 57Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al - 0.05Zr - 0.006B Consumable Electrode Remelted or Vacuum Induction Melted 1825 to 1900 °F (996 to 1038 °C) Solution, Stabilization, and P
  • 2013 SAE AMS5707L-2013 Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 58Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al - 0.05Zr - 0.006B Consumable Electrode Remelted or Vacuum Induction Melted 1825 to 1900 °F (996 to 1038 °C) Solution, Stabilizat...
  • 2008 SAE AMS5707L-2008 Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 58Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al - 0.05Zr - 0.006B Consumable Electrode Remelted or Vacuum Induction Melted 1825 to 1900 degrees F (996 to 1038 Degrees C) Solution, Stabi
  • 2007 SAE AMS5707K-2007 Nickel Alloy, Corrosion and Heat Resistant, Bars, Forgings and Rings 58Ni 19.5Cr 13.5Co 4.3Mo 3.0Ti 1.4Al 0.05Zr 0.006B Consumable Electrode or Vacuum Induction Melted 1825 to 1900°F (996 to 1038°C) Solution, Stabilization, and Precipitation Heat Treated
  • 2000 SAE AMS5707J-2000 Nickel Alloy, Corrosion and Heat Resistant, Bars, Forgings and Rings 58Ni 19.5Cr 13.5Co 4.3Mo 3.0Ti 1.4Al 0.05Zr 0.006B Consumable Electrode or Vacuum Induction Melted 1825 to 1900°F (996 to 1038°C) Solution, Stabilization, and Precipitation Heat Treated
  • 1994 SAE AMS5707H-1994 Nickel Alloy@ Corrosion and Heat Resistant@ Bars@ Forgings@ and Rings 58Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al - 0.05Zr - 0.006B Consumable Electrode or Vacuum Induction Melted 1825 to 1900 Degrees F (996 to 1038 Degrees C) Solution@ Stabilization@
  • 1989 SAE AMS5707G-1989 ALLOY BARS@ FORGINGS@ AND RINGS@ CORROSION AND HEAT RESISTANT 58Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al - 0.05Zr - 0.006B Consumable Electrode or Vacuum Induction Melted 1825? - 1900?F (996? - 1038?C) Solution@ Stabilization@ and Precipitation Heat T
  • 1981 SAE AMS5707F-1981 ALLOY BARS, FORGINGS, AND RINGS, CORROSION AND HEAT RESISTANT 58Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al - 0.05Zr - 0.006B Consumable Electrode or Vacuum Induction Melted 1825° - 1900° F (995° - 1035° C) Solution, Stabilization, and Precip...
  • 1974 SAE AMS5707E-1974 ALLOY BARS, FORGINGS, AND RINGS, CORROSION AND HEAT RESISTANT 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al - 58Ni Consumable Electrode or Vacuum Induction Melted 1825 - 1900° F (996.1 - 1037.8° C) Solution, Stabilization, and Precipitation Heat Treated
  • 1973 SAE AMS5707D-1973 ALLOY BARS, FORGINGS, AND RINGS, CORROSION AND HEAT RESISTANT Nickel Base - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al Consumable Electrode or Vacuum Induction Melted 1825 - 1900° F (996.1 - 1037.8° C) Solution, Stabilization, and Precipitation Heat Treated
  • 1970 SAE AMS5707C-1970 ALLOY BARS, FORGINGS, AND RINGS, CORROSION AND HEAT RESISTANT Nickel Base - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al Consumable Electrode or Vacuum Induction Melted 1825 - 1900 F (996.1 - 1037.8 C) Solution, Stabilization, and Precipitation Heat Treated
  • 1966 SAE AMS5707B-1966 ALLOY BARS, FORGINGS, AND RINGS, CORROSION AND HEAT RESISTANT Nickel Base - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al Solution, Stabilization, and Precipitation Heat Treated 1825 - 1900 F (996.1 - 1037.8 C) Treatment Consumable Electrode or Vacuum I...
  • 1964 SAE AMS5707A-1964 ALLOY BARS, FORGINGS, AND RINGS, CORROSION AND HEAT RESISTANT Nickel Base - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al Solution, Stabilization, and Precipitation Heat Treated 1825 - 1900 F (996.1 - 1037.8 C) Treatment Consumable Electrode or Vacuum I...
  • 1963 SAE AMS5707-1963 ALLOY BARS, FORGINGS, AND RINGS, CORROSION AND HEAT RESISTANT Nickel Base - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al Solution, Stabilization, and Precipitation Heat Treated 1825 - 1900 F (996.1 - 1037.8 C) Treatment Consumable Electrode or Vacuum I...



Copyright ©2024 All Rights Reserved