SAE AMS5707N-2017
Nickel Alloy@ Corrosion and Heat-Resistant@ Bars@ Forgings@ and Rings 57Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al - 0.05Zr - 0.006B Consumable Electrode Remelted or Vacuum Induction Melted 1825 to 1900 °F (996 to 1038 °C) Solution@ Stabilization@ and P