SAE AMS5706K-2002
Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 57Ni 19.5Cr 13.5Co 4.3Mo 3.0Ti 1.4Al 0.006B 0.05Zr Consumable Electrode or Vacuum Induction Melted 1825 to 1900°F Solution Heat Treated

Standard No.
SAE AMS5706K-2002
Release Date
2002
Published By
Society of Automotive Engineers (SAE)
Status
Replace By
SAE AMS5706L-2008
Latest
SAE AMS5706N-2020
Scope
This specification covers a corrosion and heat resistant nickel alloy in the form of bars, forgings, flash welded rings, and stock for forging, flash welded rings, or heading procured in inch/pound units. MAM 5706 is the metric version of this AMS. These products have been used typically for parts, such as fasteners, flanges, and rings, requiring high strength up to 1500 degrees F and oxidation resistance up to 1750 degrees F, particularly those parts which are formed or welded and then heat treated to develop required properties, but usage is not limited to such applications.

SAE AMS5706K-2002 history

  • 2020 SAE AMS5706N-2020 Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 57Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al - 0.006B - 0.05Zr Consumable Electrode or Vacuum Induction Melted 1825 to 1900 °F Solution Heat Treated
  • 2015 SAE AMS5706M-2015 Nickel Alloy@ Corrosion and Heat-Resistant@ Bars@ Forgings@ and Rings 57Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al - 0.006B - 0.05Zr Consumable Electrode or Vacuum Induction Melted 1825 to 1900 ��Solution Heat Treated (UNS N07001)
  • 2011 SAE AMS5706H-2011 ALLOY BARS, FORGINGS, AND RINGS, CORROSION AND HEAT RESISTANT 57Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al - 0.006B - 0.05Zr Consumable Electrode or Vacuum Induction Melted 1825° - 1900°F Solution Heat Treated
  • 2008 SAE AMS5706L-2008 Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 57Ni 19.5Cr 13.5Co 4.3Mo 3.0Ti 1.4Al 0.006B 0.05Zr Consumable Electrode or Vacuum Induction Melted 1825 to 1900°F Solution Heat Treated
  • 2002 SAE AMS5706K-2002 Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 57Ni 19.5Cr 13.5Co 4.3Mo 3.0Ti 1.4Al 0.006B 0.05Zr Consumable Electrode or Vacuum Induction Melted 1825 to 1900°F Solution Heat Treated
  • 1996 SAE AMS5706J-1996 Nickel Alloy@ Corrosion and Heat Resistant@ Bars@ Forgings@ and Rings 57Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al - 0.006B - 0.05Zr Consumable Electrode or Vacuum Induction Melted 1825 to 1900 Degrees F Solution Heat Treated (UNS N07001)
  • 1987 SAE AMS5706G-1987 ALLOY BARS@ FORGINGS@ AND RINGS@ CORROSION AND HEAT RESISTANT 57Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al - 0.006B - 0.05Zr Consumable Electrode or Vacuum Induction Melted 1825° - 1900°F Solution Heat Treated (UNS N07001)
  • 1982 SAE AMS5706F-1982 ALLOY BARS, FORGINGS, AND RINGS, CORROSION AND HEAT RESISTANT 57Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al - 0.006B - 0.05Zr Consumable Electrode or Vacuum Induction Melted 1825° - 1900°F (995° - 1040°C) Solution Heat Treated
  • 1976 SAE AMS5706E-1976 ALLOY BARS, FORGINGS, AND RINGS, CORROSION AND HEAT RESISTANT 57Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al - 0.05Zr - 0.006B Consumable Electrode or Vacuum Induction Melted 1825° - 1900° F (996° - 1038° C) Solution Heat Treated
  • 1970 SAE AMS5706D-1970 ALLOY BARS, FORGINGS, AND RINGS, CORROSION AND HEAT RESISTANT Nickel Base - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al Consumable Electrode or Vacuum Induction Melted 1825 - 1900 F (996.1 - 1037.8 C) Solution Heat Treated
  • 1968 SAE AMS5706C-1968 ALLOY BARS, FORGINGS, AND RINGS, CORROSION AND HEAT RESISTANT Nickel Base - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al Consumable Electrode or Vacuum Induction Melted 1825 - 1900 F (996.1 - 1037.8 C) Solution Heat Treated
  • 1966 SAE AMS5706B-1966 ALLOY BARS@ FORGINGS@ AND RINGS@ CORROSION AND HEAT RESISTANT Nickel Base - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al Solution Heat Treated@ 1825 - 1900 F (996.1 - 1037.8 C) Treatment Consumable Electrode or Vacuum Induction Melted
  • 1965 SAE AMS5706A-1965 ALLOY BARS, FORGINGS, AND RINGS, CORROSION AND HEAT RESISTANT Nickel Base - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al Solution Heat Treated, 1825 - 1900 F (996.1 - 1037.8 C) Treatment Consumable Electrode or Vacuum Induction Melted