SAE AMS5706J-1996
Nickel Alloy@ Corrosion and Heat Resistant@ Bars@ Forgings@ and Rings 57Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al - 0.006B - 0.05Zr Consumable Electrode or Vacuum Induction Melted 1825 to 1900 Degrees F Solution Heat Treated (UNS N07001)

Standard No.
SAE AMS5706J-1996
Release Date
1996
Published By
SAE - SAE International
Status
Replace By
SAE AMS5706K-2002
Latest
SAE AMS5706N-2020

SAE AMS5706J-1996 history

  • 2020 SAE AMS5706N-2020 Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 57Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al - 0.006B - 0.05Zr Consumable Electrode or Vacuum Induction Melted 1825 to 1900 °F Solution Heat Treated
  • 2015 SAE AMS5706M-2015 Nickel Alloy@ Corrosion and Heat-Resistant@ Bars@ Forgings@ and Rings 57Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al - 0.006B - 0.05Zr Consumable Electrode or Vacuum Induction Melted 1825 to 1900 ��Solution Heat Treated (UNS N07001)
  • 2011 SAE AMS5706H-2011 ALLOY BARS, FORGINGS, AND RINGS, CORROSION AND HEAT RESISTANT 57Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al - 0.006B - 0.05Zr Consumable Electrode or Vacuum Induction Melted 1825° - 1900°F Solution Heat Treated
  • 2008 SAE AMS5706L-2008 Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 57Ni 19.5Cr 13.5Co 4.3Mo 3.0Ti 1.4Al 0.006B 0.05Zr Consumable Electrode or Vacuum Induction Melted 1825 to 1900°F Solution Heat Treated
  • 2002 SAE AMS5706K-2002 Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 57Ni 19.5Cr 13.5Co 4.3Mo 3.0Ti 1.4Al 0.006B 0.05Zr Consumable Electrode or Vacuum Induction Melted 1825 to 1900°F Solution Heat Treated
  • 1996 SAE AMS5706J-1996 Nickel Alloy@ Corrosion and Heat Resistant@ Bars@ Forgings@ and Rings 57Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al - 0.006B - 0.05Zr Consumable Electrode or Vacuum Induction Melted 1825 to 1900 Degrees F Solution Heat Treated (UNS N07001)
  • 1987 SAE AMS5706G-1987 ALLOY BARS@ FORGINGS@ AND RINGS@ CORROSION AND HEAT RESISTANT 57Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al - 0.006B - 0.05Zr Consumable Electrode or Vacuum Induction Melted 1825° - 1900°F Solution Heat Treated (UNS N07001)
  • 1982 SAE AMS5706F-1982 ALLOY BARS, FORGINGS, AND RINGS, CORROSION AND HEAT RESISTANT 57Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al - 0.006B - 0.05Zr Consumable Electrode or Vacuum Induction Melted 1825° - 1900°F (995° - 1040°C) Solution Heat Treated
  • 1976 SAE AMS5706E-1976 ALLOY BARS, FORGINGS, AND RINGS, CORROSION AND HEAT RESISTANT 57Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al - 0.05Zr - 0.006B Consumable Electrode or Vacuum Induction Melted 1825° - 1900° F (996° - 1038° C) Solution Heat Treated
  • 1970 SAE AMS5706D-1970 ALLOY BARS, FORGINGS, AND RINGS, CORROSION AND HEAT RESISTANT Nickel Base - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al Consumable Electrode or Vacuum Induction Melted 1825 - 1900 F (996.1 - 1037.8 C) Solution Heat Treated
  • 1968 SAE AMS5706C-1968 ALLOY BARS, FORGINGS, AND RINGS, CORROSION AND HEAT RESISTANT Nickel Base - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al Consumable Electrode or Vacuum Induction Melted 1825 - 1900 F (996.1 - 1037.8 C) Solution Heat Treated
  • 1966 SAE AMS5706B-1966 ALLOY BARS@ FORGINGS@ AND RINGS@ CORROSION AND HEAT RESISTANT Nickel Base - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al Solution Heat Treated@ 1825 - 1900 F (996.1 - 1037.8 C) Treatment Consumable Electrode or Vacuum Induction Melted
  • 1965 SAE AMS5706A-1965 ALLOY BARS, FORGINGS, AND RINGS, CORROSION AND HEAT RESISTANT Nickel Base - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al Solution Heat Treated, 1825 - 1900 F (996.1 - 1037.8 C) Treatment Consumable Electrode or Vacuum Induction Melted
  • 1964 SAE AMS5706-1964 ALLOY BARS, FORGINGS, AND RINGS, CORROSION AND HEAT RESISTANT Nickel Base - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al Solution Heat Treated, 1825 - 1900 F (996.1 - 1037.8 C) Treatment Consumable Electrode or Vacuum Induction Melted