SAE AMS5708M-2019
Scope
This specification covers a corrosion and heat resistant nickel alloy in the form of bars, forgings, flash welded rings, and stock for forging, flash welded rings, or heading. These products have been used typically for parts, such as bolts and turbine blades, requiring high strength up to 1500 °F (816 °C) and oxidation resistance up to 1750 °F (954 °C), but usage is not limited to such applications.

SAE AMS5708J-2006 history

  • 2019 SAE AMS5708M-2019 Nickel Alloy@ Corrosion and Heat-Resistant@ Bars@ Wire@ Forgings@ and Rings 58Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al - 0.05Zr - 0.006B Consumable Electrode or Vacuum Induction Melted 1975 °F (1079 °C) Solution Heat Treated (UNS N07001)
  • 2015 SAE AMS5708L-2015 Nickel Alloy, Corrosion and Heat-Resistant, Bars, Wire Forgings, and Rings 58Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al - 0.05Zr - 0.006B Consumable Electrode or Vacuum Induction Melted 1975 °F (1079 °C) Solution Heat Treated
  • 2008 SAE AMS5708K-2008 Nickel Alloy@ Corrosion and Heat-Resistant@ Bars@ Wire Forgings@ and Rings 58Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al Consumable Electrode or Vacuum Induction Melted 1975 °F (1079 °C) Solution Heat Treated (UNS N07001)
  • 2006 SAE AMS5708J-2006 Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 58Ni 19.5Cr 13.5Co 4.3Mo 3.0Ti 1.4Al Consumable Electrode or Vacuum Induction Melted 1975°F (1079°C) Solution Heat Treated
  • 2002 SAE AMS5708H-2002 Nickel Alloy@ Corrosion and Heat-Resistant@ Bars@ Forgings@ and Rings 58Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4AI Consumable Electrode or Vacuum Induction Melted 1975 °F (1079 °C) Solution Heat Treated
  • 1995 SAE AMS5708G-1995 Nickel Alloy@ Corrosion and Heat Resistant@ Bars@ Forgings@ and Rings 58Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al Consumable Electrode or Vacuum Induction Melted 1975 Degrees F (1079 Degrees C) Solution Heat Treated (UNS N07001)
  • 1990 SAE AMS5708F-1990 ALLOY BARS, FORGINGS AND RINGS, CORROSION AND HEAT RESISTANT 58Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al Consumable Electrode or Vacuum Induction Melted 1975°F (1079°C) Solution Heat Treated
  • 1981 SAE AMS5708E-1981 ALLOY BARS AND FORGINGS, CORROSION AND HEAT RESISTANT 58Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al Consumable Electrode or Vacuum Induction Melted 1975°F (1080°C) Solution Heat Treated
  • 1981 SAE AMS5708D-1981 ALLOY BARS AND FORGINGS@ CORROSION AND HEAT RESISTANT 58Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al Consumable Electrode or Vacuum Induction Melted 1975 Degrees F (1080 Degrees C) Solution Heat Treated (UNS N07001)
  • 1973 SAE AMS5708C-1973 ALLOY BARS AND FORGINGS@ CORROSION AND HEAT RESISTANT Nickel Base - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al Consumable Electrode or Vacuum Induction Melted 1975 Degrees F (1079.4 Degrees C) Solution Heat Treated
  • 1970 SAE AMS5708B-1970 ALLOY BARS AND FORGINGS@ CORROSION AND HEAT RESISTANT Nickel Base - 19.Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al Consumable Electrode or Vacuum Induction Melted 1975 F (1079.4 C) Solution Heat Treated
  • 1970 SAE AMS5708A-1970 ALLOY BARS AND FORGINGS@ CORROSION AND HEAT RESISTANT Nickel Base - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al Consumable Electrode or Vacuum Induction Melted 1975 F (1079.4 C) Solution Heat Treated
  • 1963 SAE AMS5708-1963 ALLOY BARS AND FORGINGS@ CORROSION AND HEAT RESISTANT Nickel Base - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al Solution Heat Treated@ 1975 F (1079.4 C)Treatment consumable Electrode or Vacuum Induction Melted



Copyright ©2024 All Rights Reserved