Scope
This specification covers a corrosion and heat-resistant nickel alloy in the form of bars, wire, forgings, flash welded rings, and stock for forging, flash welded rings, or heading.

SAE AMS5708L-2015 history

  • 2019 SAE AMS5708M-2019 Nickel Alloy@ Corrosion and Heat-Resistant@ Bars@ Wire@ Forgings@ and Rings 58Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al - 0.05Zr - 0.006B Consumable Electrode or Vacuum Induction Melted 1975 °F (1079 °C) Solution Heat Treated (UNS N07001)
  • 2015 SAE AMS5708L-2015 Nickel Alloy, Corrosion and Heat-Resistant, Bars, Wire Forgings, and Rings 58Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al - 0.05Zr - 0.006B Consumable Electrode or Vacuum Induction Melted 1975 °F (1079 °C) Solution Heat Treated
  • 2008 SAE AMS5708K-2008 Nickel Alloy@ Corrosion and Heat-Resistant@ Bars@ Wire Forgings@ and Rings 58Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al Consumable Electrode or Vacuum Induction Melted 1975 °F (1079 °C) Solution Heat Treated (UNS N07001)
  • 2006 SAE AMS5708J-2006 Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 58Ni 19.5Cr 13.5Co 4.3Mo 3.0Ti 1.4Al Consumable Electrode or Vacuum Induction Melted 1975°F (1079°C) Solution Heat Treated
  • 2002 SAE AMS5708H-2002 Nickel Alloy@ Corrosion and Heat-Resistant@ Bars@ Forgings@ and Rings 58Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4AI Consumable Electrode or Vacuum Induction Melted 1975 °F (1079 °C) Solution Heat Treated
  • 1995 SAE AMS5708G-1995 Nickel Alloy@ Corrosion and Heat Resistant@ Bars@ Forgings@ and Rings 58Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al Consumable Electrode or Vacuum Induction Melted 1975 Degrees F (1079 Degrees C) Solution Heat Treated (UNS N07001)
  • 1990 SAE AMS5708F-1990 ALLOY BARS, FORGINGS AND RINGS, CORROSION AND HEAT RESISTANT 58Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al Consumable Electrode or Vacuum Induction Melted 1975°F (1079°C) Solution Heat Treated
  • 1981 SAE AMS5708E-1981 ALLOY BARS AND FORGINGS, CORROSION AND HEAT RESISTANT 58Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al Consumable Electrode or Vacuum Induction Melted 1975°F (1080°C) Solution Heat Treated
  • 1981 SAE AMS5708D-1981 ALLOY BARS AND FORGINGS@ CORROSION AND HEAT RESISTANT 58Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al Consumable Electrode or Vacuum Induction Melted 1975 Degrees F (1080 Degrees C) Solution Heat Treated (UNS N07001)
  • 1973 SAE AMS5708C-1973 ALLOY BARS AND FORGINGS@ CORROSION AND HEAT RESISTANT Nickel Base - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al Consumable Electrode or Vacuum Induction Melted 1975 Degrees F (1079.4 Degrees C) Solution Heat Treated
  • 1970 SAE AMS5708B-1970 ALLOY BARS AND FORGINGS@ CORROSION AND HEAT RESISTANT Nickel Base - 19.Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al Consumable Electrode or Vacuum Induction Melted 1975 F (1079.4 C) Solution Heat Treated
  • 1970 SAE AMS5708A-1970 ALLOY BARS AND FORGINGS@ CORROSION AND HEAT RESISTANT Nickel Base - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al Consumable Electrode or Vacuum Induction Melted 1975 F (1079.4 C) Solution Heat Treated
  • 1963 SAE AMS5708-1963 ALLOY BARS AND FORGINGS@ CORROSION AND HEAT RESISTANT Nickel Base - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al Solution Heat Treated@ 1975 F (1079.4 C)Treatment consumable Electrode or Vacuum Induction Melted