Scope
This specification covers a blend of tungsten carbide-cobalt aggregate, a nickel alloy, and a nickel aluminum aggregate in the form of powder. This product has been used typically for producing plasma spray coatings to provide surfaces resistant to wear, corrosion, and abrasion, but usage is not limited to such applications.

SAE AMS5792B-2006 Referenced Document

  • ASTM B214-99 Standard Test Method for Sieve Analysis of Metal Powders
  • ASTM B215-04 Standard Practices for Sampling Metal Powders*2024-04-18 Update

SAE AMS5792B-2006 history

  • 2024 SAE AMS5792C-2024 Powder, Plasma Spray 50 (88WC - 12Co) + 35 (70Ni - 16.5Cr - 4Fe - 4Si - 3.8B) + 15 (80Ni - 20Al) Three-Component Mixture
  • 2018 SAE AMS5792B-2018 Powder, Plasma Spray 50 (88WC - 12Co) + 35 (70Ni - 16.5Cr - 4Fe - 4Si - 3.8B) + 15 (80Ni - 20A1) Three-Component Mixture
  • 2011 SAE AMS5792-2011 POWDER, PLASMA SPRAY 50(88W - 12Co) + 35(70Ni - 16.5Cr - 4Fe - 4Si - 3.8B) + 15(80Ni - 20Al) Three-Component Mixture
  • 2006 SAE AMS5792B-2006 Powder, Plasma Spray 50 (88WC - 12Co) + 35 (70Ni - 16.5Cr - 4Fe - 4Si - 3.8B) + 15 (80Ni - 20A1) Three-Component Mixture
  • 1998 SAE AMS5792A-1998 Powder, Plasma Spray 50 (88WC - 12Co) + 35 (70Ni - 16.5Cr - 4Fe - 4Si - 3.8B) + 15 (80Ni - 20A1) Three-Component Mixture
  • 1992 SAE AMS5792A-1992 Powder, Plasma Spray 50(88W 12Co) + 35(70Ni 16.5Cr 4Fe 4Si 3.8B) + 15(80Ni 20Al) Three-Component Mixture



Copyright ©2024 All Rights Reserved