Scope
This specification establishes requirements and procedures for generating nitrided surfaces on steel parts using a process controlled by the nitriding potential. The nitriding process described herein is used typically to produce a nitride case on carbon and alloy steels, tool steels, nitriding steels, corrosion resistant steels and other ferrous alloys. Applicable, allowance should be made for growth.

SAE AMS2759/10A-2006 Referenced Document

  • ASTM E140-05 Standard Hardness Conversion Tables for Metals Relationship Among Brinell Hardness, Vickers Hardness, Rockwell Hardness, Superficial Hardness, Knoop Hardness, and Scleroscope Hardness*2024-04-18 Update
  • ASTM E384-05 Standard Test Method for Microindentation Hardness of Materials
  • ASTM E384-06 Standard Test Method for Microindentation Hardness of Materials*2024-04-18 Update
  • SAE AMS2418G-2006 Plating, Copper
  • SAE AMS2429 BRONZE PLATE MASKING*2011-08-10 Update
  • SAE AMS2750D-2005 (R) Pyrometry
  • SAE AMS2759D-2006 Heat Treatment of Steel Parts General Requirements
  • SAE ARP1820-1984 Chord Method of Evaluating Surface Microstructural Characteristics
  • SAE ARP1820A-1997 Chord Method of Evaluating Surface Microstructural Characteristics

SAE AMS2759/10A-2006 history


SAE AMS2759/10A-2006 -All Parts

SAE AMS2759-1984 HEAT TREATMENT OF STEEL PARTS General Requirements SAE AMS2759/1-1994 Heat Treatment of Carbon and Low-Alloy Steel Parts, Minimum Tensile Strength Below 220 ksi (1517 MPa) SAE AMS2759/10-1999 Automated Gaseous Nitriding Controlled by Nitriding Potential SAE AMS2759/10A-2014 Automated Gaseous Nitriding Controlled by Nitriding Potential SAE AMS2759/10B-2018 Automated Gaseous Nitriding Controlled by Nitriding Potential SAE AMS2759/11-2014 Stress Relief of Steel Parts SAE AMS2759/11A-2018 Stress Relief of Steel Parts SAE AMS2759/12-2007 Gaseous Nitrocarburizing@ Automatically Controlled by Potentials SAE AMS2759/12A-2007 Gaseous Nitrocarburizing, Automatically Controlled by Potentials SAE AMS2759/12B-2018 Gaseous Nitrocarburizing, Automatically Controlled by Potentials SAE AMS2759/13-2018 Gaseous Nitrocarburizing SAE AMS2759/1A-1996 Heat Treatment of Carbon and Low-Alloy Steel Parts Minimum Tensile Strength Below 220 ksi (1517 MPa) SAE AMS2759/1B-1996 Heat Treatment of Carbon and Low-Alloy Steel Parts Minimum Tensile Strength Below 220 ksi (1517 MPa) SAE AMS2759/1C-2000 Heat Treatment of Carbon and Low-Alloy Steel Parts Minimum Tensile Strength Below 220 ksi (1517 MPa) SAE AMS2759/1D-2007 Heat Treatment of Carbon and Low-Alloy Steel Parts Minimum Tensile Strength Below 220 ksi (1517 MPa) SAE AMS2759/1E-2014 Heat Treatement of Carbon and Low-Alloy Steel Parts Minimum Tensile Strength Below 220 ksi (1517 MPa) SAE AMS2759/1F-2018 Heat Treatment of Carbon and Low-Alloy Steel Parts Minimum Tensile Strength Below 220 ksi (1517 MPa) SAE AMS2759/1G-2019 Heat Treatment of Carbon and Low-Alloy Steel Parts Minimum Tensile Strength Below 220 ksi (1517 MPa) SAE AMS2759/1H-2019 Heat Treatment of Carbon and Low-Alloy Steel Parts Minimum Tensile Strength Below 220 ksi (1517 MPa) SAE AMS2759/1J-2021 Heat Treatment of Carbon and Low-Alloy Steel Parts Minimum Tensile Strength Below 220 ksi (1517 MPa) SAE AMS2759/2-2011 Heat Treatment of Low-Alloy Steel Parts Minimum Tensile Strength 220 ksi (1517 MPa) and Higher SAE AMS2759/2A-1996 Heat Treatment of Low-Alloy Steel Parts Minimum Tensile Strength 220 ksi (1517 MPa) and Higher SAE AMS2759/2B-1996 Heat Treatment of Low-Alloy Steel Parts Minimum Tensile Strength 220 ksi (1517 MPa) and Higher SAE AMS2759/2C-2000 Heat Treatment of Low-Alloy Steel Parts Minimum Tensile Strength 220 Ksi (1517 MPa) and Higher SAE AMS2759/2D-2007 Heat Treatment of Low-Alloy Steel Parts Minimum Tensile Strength 220 ksi (1517 MPa) and Higher SAE AMS2759/2E-2009 Heat Treatment of Low-Alloy Steel Parts Minimum Tensile Strength 220 ksi (1517 MPa) and Higher SAE AMS2759/2F-2014 Heat Treatment of Low-Alloy Steel Parts Minimum Tensile Strength 220 ksi (1517 MPa) and Higher SAE AMS2759/2G-2018 Heat Treatment of Low-Alloy Steel Parts Minimum Tensile Strength 220 ksi (1517 MPa) and Higher SAE AMS2759/2H-2018 Heat Treatment of Low-Alloy Steel Parts Minimum Tensile Strength 220 ksi (1517 MPa) and Higher SAE AMS2759/2J-2019 Heat Treatment of Low-Alloy Steel Parts Minimum Tensile Strength 220 ksi (1517 MPa) and Higher SAE AMS2759/2K-2021 Heat Treatment of Low-Alloy Steel Parts Minimum Tensile Strength 220 ksi (1517 MPa) and Higher SAE AMS2759/3-2011 Heat Treatment, Precipitation-Hardening Corrosion-Resistant and Maraging Steel Parts SAE AMS2759/3A-1996 Heat Treatment Precipitation-Hardening Corrosion-Resistant and Maraging Steel Parts SAE AMS2759/3B-1996 Heat Treatment Precipitation-Hardening Corrosion-Resistant and Maraging Steel Parts SAE AMS2759/3C-2000 Heat Treatment Precipitation-Hardening Corrosion-Resistant and Maraging Steel Parts SAE AMS2759/3D-2005 Heat Treatment Precipitation-Hardening Corrosion-Resistant and Maraging Steel Parts SAE AMS2759/3E-2014 Heat Treatment Precipitation-Hardening Corrosion-Resistant and Maraging Steel parts SAE AMS2759/3F-2015 Heat Treatment Precipitation-Hardening Corrosion-Resistant and Maraging Steel Parts SAE AMS2759/3G-2018 Heat Treatment Precipitation-Hardening Corrosion-Resistant and Maraging Steel Parts SAE AMS2759/3H-2019 Heat Treatment Precipitation-Hardening Corrosion-Resistant, Maraging, and Secondary Hardening Steel Parts SAE AMS2759/3J-2020 Heat Treatment Precipitation-Hardening Corrosion-Resistant, Maraging, and Secondary Hardening Steel Parts SAE AMS2759/4-2011 Heat Treatment, Austenitic Corrosion-Resistant Steel Parts SAE AMS2759/4A-1996 HEAT TREATMENT AUSTENITIC CORROSION-RESISTANT STEEL PARTS



Copyright ©2024 All Rights Reserved