SAE AMS2759/12B-2018
Gaseous Nitrocarburizing, Automatically Controlled by Potentials

Standard No.
SAE AMS2759/12B-2018
Release Date
2018
Published By
SAE - SAE International
Latest
SAE AMS2759/12B-2018
Scope
Purpose This specification covers the requirements for producing a continuous white layer with controlled extent of porosity by means of a gaseous process@ automatically controlled to maintain set values of the nitriding and carburizing potentials that determine properties of the nitrocarburized surface. Automatic control is intended to ensure repeatability of nitrogen and carbon content of the white layer which influences properties such as wear and corrosion resistance@ ductility and fatigue strength. Application The nitrocarburizing process described herein is used typically for enhancement of wear resistance and fatigue strength@ as well as corrosion resistance in ferrous alloys but usage is not limited to such applications. The provisions of this specification revision shall become effective 90 days after publication. Safety ?C Hazardous Materials While the materials@ methods@ applications@ and processes described or referenced in this specification may involve the use of hazardous materials@ this specification does not address the hazards which may be involved in such use. It is the responsibility of the user to ensure familiarity with the safe and proper use of any hazardous materials and to take necessary precautionary measures to ensure the health and safety of all personnel involved.

SAE AMS2759/12B-2018 history

Gaseous Nitrocarburizing, Automatically Controlled by Potentials

SAE AMS2759/12B-2018 -All Parts

SAE AMS2759-1984 HEAT TREATMENT OF STEEL PARTS General Requirements SAE AMS2759/1-1994 Heat Treatment of Carbon and Low-Alloy Steel Parts, Minimum Tensile Strength Below 220 ksi (1517 MPa) SAE AMS2759/10-1999 Automated Gaseous Nitriding Controlled by Nitriding Potential SAE AMS2759/10A-2014 Automated Gaseous Nitriding Controlled by Nitriding Potential SAE AMS2759/10B-2018 Automated Gaseous Nitriding Controlled by Nitriding Potential SAE AMS2759/11-2014 Stress Relief of Steel Parts SAE AMS2759/11A-2018 Stress Relief of Steel Parts SAE AMS2759/12-2007 Gaseous Nitrocarburizing@ Automatically Controlled by Potentials SAE AMS2759/12A-2007 Gaseous Nitrocarburizing, Automatically Controlled by Potentials SAE AMS2759/12B-2018 Gaseous Nitrocarburizing, Automatically Controlled by Potentials SAE AMS2759/13-2018 Gaseous Nitrocarburizing SAE AMS2759/1A-1996 Heat Treatment of Carbon and Low-Alloy Steel Parts Minimum Tensile Strength Below 220 ksi (1517 MPa) SAE AMS2759/1B-1996 Heat Treatment of Carbon and Low-Alloy Steel Parts Minimum Tensile Strength Below 220 ksi (1517 MPa) SAE AMS2759/1C-2000 Heat Treatment of Carbon and Low-Alloy Steel Parts Minimum Tensile Strength Below 220 ksi (1517 MPa) SAE AMS2759/1D-2007 Heat Treatment of Carbon and Low-Alloy Steel Parts Minimum Tensile Strength Below 220 ksi (1517 MPa) SAE AMS2759/1E-2014 Heat Treatement of Carbon and Low-Alloy Steel Parts Minimum Tensile Strength Below 220 ksi (1517 MPa) SAE AMS2759/1F-2018 Heat Treatment of Carbon and Low-Alloy Steel Parts Minimum Tensile Strength Below 220 ksi (1517 MPa) SAE AMS2759/1G-2019 Heat Treatment of Carbon and Low-Alloy Steel Parts Minimum Tensile Strength Below 220 ksi (1517 MPa) SAE AMS2759/1H-2019 Heat Treatment of Carbon and Low-Alloy Steel Parts Minimum Tensile Strength Below 220 ksi (1517 MPa) SAE AMS2759/1J-2021 Heat Treatment of Carbon and Low-Alloy Steel Parts Minimum Tensile Strength Below 220 ksi (1517 MPa) SAE AMS2759/2-2011 Heat Treatment of Low-Alloy Steel Parts Minimum Tensile Strength 220 ksi (1517 MPa) and Higher SAE AMS2759/2A-1996 Heat Treatment of Low-Alloy Steel Parts Minimum Tensile Strength 220 ksi (1517 MPa) and Higher SAE AMS2759/2B-1996 Heat Treatment of Low-Alloy Steel Parts Minimum Tensile Strength 220 ksi (1517 MPa) and Higher SAE AMS2759/2C-2000 Heat Treatment of Low-Alloy Steel Parts Minimum Tensile Strength 220 Ksi (1517 MPa) and Higher SAE AMS2759/2D-2007 Heat Treatment of Low-Alloy Steel Parts Minimum Tensile Strength 220 ksi (1517 MPa) and Higher SAE AMS2759/2E-2009 Heat Treatment of Low-Alloy Steel Parts Minimum Tensile Strength 220 ksi (1517 MPa) and Higher SAE AMS2759/2F-2014 Heat Treatment of Low-Alloy Steel Parts Minimum Tensile Strength 220 ksi (1517 MPa) and Higher SAE AMS2759/2G-2018 Heat Treatment of Low-Alloy Steel Parts Minimum Tensile Strength 220 ksi (1517 MPa) and Higher SAE AMS2759/2H-2018 Heat Treatment of Low-Alloy Steel Parts Minimum Tensile Strength 220 ksi (1517 MPa) and Higher SAE AMS2759/2J-2019 Heat Treatment of Low-Alloy Steel Parts Minimum Tensile Strength 220 ksi (1517 MPa) and Higher SAE AMS2759/2K-2021 Heat Treatment of Low-Alloy Steel Parts Minimum Tensile Strength 220 ksi (1517 MPa) and Higher SAE AMS2759/3-2011 Heat Treatment, Precipitation-Hardening Corrosion-Resistant and Maraging Steel Parts SAE AMS2759/3A-1996 Heat Treatment Precipitation-Hardening Corrosion-Resistant and Maraging Steel Parts SAE AMS2759/3B-1996 Heat Treatment Precipitation-Hardening Corrosion-Resistant and Maraging Steel Parts SAE AMS2759/3C-2000 Heat Treatment Precipitation-Hardening Corrosion-Resistant and Maraging Steel Parts SAE AMS2759/3D-2005 Heat Treatment Precipitation-Hardening Corrosion-Resistant and Maraging Steel Parts SAE AMS2759/3E-2014 Heat Treatment Precipitation-Hardening Corrosion-Resistant and Maraging Steel parts SAE AMS2759/3F-2015 Heat Treatment Precipitation-Hardening Corrosion-Resistant and Maraging Steel Parts SAE AMS2759/3G-2018 Heat Treatment Precipitation-Hardening Corrosion-Resistant and Maraging Steel Parts SAE AMS2759/3H-2019 Heat Treatment Precipitation-Hardening Corrosion-Resistant, Maraging, and Secondary Hardening Steel Parts SAE AMS2759/3J-2020 Heat Treatment Precipitation-Hardening Corrosion-Resistant, Maraging, and Secondary Hardening Steel Parts SAE AMS2759/4-2011 Heat Treatment, Austenitic Corrosion-Resistant Steel Parts SAE AMS2759/4A-1996 HEAT TREATMENT AUSTENITIC CORROSION-RESISTANT STEEL PARTS



Copyright ©2024 All Rights Reserved