SAE AMS5853C-2006
Steel, Corrosion and Heat Resistant, Bars and Wire 15Cr - 25.5Ni - 1.2Mo - 2.1Ti - 0.006B - 0.30V Consumable Electrode Melted 1800 Degrees F (982 Degrees C) Solution Treated and Work-Strengthened 160 ksi (1103 MPa) Tensile Strength UNS S66286

Standard No.
SAE AMS5853C-2006
Release Date
2006
Published By
Society of Automotive Engineers (SAE)
Status
Replace By
SAE AMS5853C-2012
Latest
SAE AMS5853E-2024
Scope
This specification covers a corrosion and heat resistant steel in the form of work-strengthened bars and wire 1-1/4 inches (31.8 mm) and under in nominal diameter or least distance between parallel sides. These bars and wire have been used typically for parts, such as fasteners, requiring room- temperature minimum tensile strength of 160 ksi (1103 MPa) after precipitation heat treatment for use up to 1000 °F (538 °C) and having oxidation resistance up to 1200 °F (649 °C), but usage is not limited to such applications.

SAE AMS5853C-2006 Referenced Document

  • ASTM A370-05 Standard Test Methods and Definitions for Mechanical Testing of Steel Products*2024-04-18 Update
  • ASTM A370-06 Standard Test Methods and Definitions for Mechanical Testing of Steel Products*2024-04-18 Update
  • SAE AMS2241P-2005 Tolerances Corrosion and Heat Resistant Steel, Iron Alloy, Titanium, and Titanium Alloy Bars and Wire
  • SAE AMS2248F-2006 Chemical Check Analysis Limits Corrosion and Heat Resistant Steels and Alloys, Maraging and Other Highly-Alloyed Steels, and Iron Alloys
  • SAE AMS2371G-2003 Quality Assurance Sampling and Testing Corrosion and Heat-Resistant Steels and Alloys Wrought Products and Forging Stock
  • SAE AMS2750D-2005 (R) Pyrometry
  • SAE AMS2806B-2000 Identification Bars, Wire, Mechanical Tubing, and Extrusions Carbon and Alloy Steels and Corrosion and Heat Resistant Steels and Alloys

SAE AMS5853C-2006 history

  • 2024 SAE AMS5853E-2024 Steel, Corrosion- and Heat-Resistant, Bars and Wire 15Cr - 25.5Ni - 1.2Mo - 2.1Ti - 0.006B - 0.30V Consumable Electrode Remelted 1800 °F (982 °C) Solution Heat Treated and Work-Strengthened 160 ksi (1103 MPa) Tensile Strength Capability
  • 2019 SAE AMS5853D-2019 Steel@ Corrosion and Heat-Resistant@ Bars and Wire 15Cr - 25.5Ni - 1.2Mo - 2.1Ti - 0.006B - 0.30V Consumable Electrode Melted 1800 °F (982 °C) Solution Treated and Work-Strengthened 160 ksi (1103 MPa) Tensile Strength (UNS S66286)
  • 2012 SAE AMS5853C-2012 Steel, Corrosion and Heat-Resistant, Bars and Wire 15Cr - 25.5Ni - 1.2Mo - 2.1Ti - 0.006B - 0.30V Consumable Electrode Melted 1800 °F (982 °C) Solution Treated and Work-Strengthened 160 ksi (1103 MPa) Tensile Strength
  • 2006 SAE AMS5853C-2006 Steel, Corrosion and Heat Resistant, Bars and Wire 15Cr - 25.5Ni - 1.2Mo - 2.1Ti - 0.006B - 0.30V Consumable Electrode Melted 1800 Degrees F (982 Degrees C) Solution Treated and Work-Strengthened 160 ksi (1103 MPa) Tensile Strength UNS S66286
  • 2000 SAE AMS5853B-2000 Steel, Corrosion and Heat Resistant, Bars and Wire 15Cr 25.5Ni 1.2Mo 2.1Ti 0.006B 0.30V, Consumable Electrode Melted 1800°F (982°C) Solution Treated and Work-Strengthened 160 ksi (1103 MPa) Tensile Strength
  • 1993 SAE AMS5853A-1993 Steel@ Corrosion and Heat Resistant@ Bars and Wire 15Cr - 25.5Ni - 1.2Mo - 2.1Ti - 0.006B - 0.30V Consumable Electrode Melted 1800 Degrees F (982 Degrees C) Solution Treated and Work-Strengthened 160 ksi (1103 MPa) Tensile Strength (UNS K66286)
  • 1991 SAE AMS5853-1991 STEEL BARS, CORROSION AND HEAT RESISTANT 15Cr - 25.5Ni - 1.2Mo - 2.1Ti - 0.006B - 0.30V 1800°F (980°C) Solution Treated and Work-Strengthened 160,000 psi (1105 MPa) Tensile Strength, Consumable Electrode Melted



Copyright ©2024 All Rights Reserved