SAE AMS5389C-1987
Alloy Castings, Sand, Corrosion and Heat Resistant, 55Ni 16.5Cr 17Mo 4.5W 5.8Fe 0.40V, Solution Heat Treated
Home
SAE AMS5389C-1987
Standard No.
SAE AMS5389C-1987
Release Date
1987
Published By
Society of Automotive Engineers (SAE)
Status
Be replaced
2017-04
Replace By
SAE AMS5389C-1994
Latest
SAE AMS5389D-2017
Scope
This specification has been declared NONCURRENT by the Aerospace Materials Division, SAE, as of November 1994. It is recommended, therefore, that this specification not be specified for new designs.
SAE AMS5389C-1987 history
2017
SAE AMS5389D-2017
Alloy Castings@ Sand@ Corrosion and Heat Resistant 55Ni - 16.5Cr - 17Mo - 4.5W - 5.8Fe - 0.40V Solution Heat Treated (UNS N10002)
2012
SAE AMS5389C-2012
Alloy Castings, Sand, Corrosion and Heat Resistant 55Ni - 16.5Cr - 17Mo - 4.5W - 5.8Fe - 0.40V Solution Heat Treated
2011
SAE AMS5389B-2011
ALLOY CASTINGS, SAND, CORROSION AND HEAT RESISTANT 55Ni - 16.5Cr - 17Mo - 4.5W - 5.8Fe - 0.40V Solution Heat Treated
1994
SAE AMS5389C-1994
Alloy Castings@ Sand@ Corrosion and Heat Resistant 55Ni - 16.5Cr - 17Mo - 4.5W - 5.8Fe - 0.40V Solution Heat Treated (UNS N10002)
1987
SAE AMS5389C-1987
Alloy Castings, Sand, Corrosion and Heat Resistant, 55Ni 16.5Cr 17Mo 4.5W 5.8Fe 0.40V, Solution Heat Treated
1951
SAE AMS5389A-1951
ALLOY CASTINGS, SAND, CORROSION AND HEAT RESISTANT Nickel Base - 17Mo - 15Cr - 6Fe - 5W
1948
SAE AMS5389-1948
ALLOY CASTINGS, SAND, CORROSION AND HEAT RESISTANT Nickel Base 17Mo - 15Cr - 6Fe - 5W
Copyright ©2024 All Rights Reserved