Scope
This specification covers a corrosion and heat resistant nickel alloy in the form of sand castings.

SAE AMS5389C-2012 history

  • 2017 SAE AMS5389D-2017 Alloy Castings@ Sand@ Corrosion and Heat Resistant 55Ni - 16.5Cr - 17Mo - 4.5W - 5.8Fe - 0.40V Solution Heat Treated (UNS N10002)
  • 2012 SAE AMS5389C-2012 Alloy Castings, Sand, Corrosion and Heat Resistant 55Ni - 16.5Cr - 17Mo - 4.5W - 5.8Fe - 0.40V Solution Heat Treated
  • 2011 SAE AMS5389B-2011 ALLOY CASTINGS, SAND, CORROSION AND HEAT RESISTANT 55Ni - 16.5Cr - 17Mo - 4.5W - 5.8Fe - 0.40V Solution Heat Treated
  • 1994 SAE AMS5389C-1994 Alloy Castings@ Sand@ Corrosion and Heat Resistant 55Ni - 16.5Cr - 17Mo - 4.5W - 5.8Fe - 0.40V Solution Heat Treated (UNS N10002)
  • 1987 SAE AMS5389C-1987 Alloy Castings, Sand, Corrosion and Heat Resistant, 55Ni 16.5Cr 17Mo 4.5W 5.8Fe 0.40V, Solution Heat Treated
  • 1951 SAE AMS5389A-1951 ALLOY CASTINGS, SAND, CORROSION AND HEAT RESISTANT Nickel Base - 17Mo - 15Cr - 6Fe - 5W
  • 1948 SAE AMS5389-1948 ALLOY CASTINGS, SAND, CORROSION AND HEAT RESISTANT Nickel Base 17Mo - 15Cr - 6Fe - 5W



Copyright ©2024 All Rights Reserved