SAE AMS5356B-2006
Steel, Corrosion Resistant, Investment Castings 15Cr - 4.6Ni - 0.22Cb - 2.8Cu Solution and Precipitation Heat Treated (H1100) 130 ksi (896 MPa) Tensile Strength

Standard No.
SAE AMS5356B-2006
Release Date
2006
Published By
Society of Automotive Engineers (SAE)
Status
Replace By
SAE AMS5356C-2010
Latest
SAE AMS5356D-2022
Scope
This specification covers a corrosion resistant steel in the form of investment castings.

SAE AMS5356B-2006 history

  • 2022 SAE AMS5356D-2022 Steel, Corrosion-Resistant, Investment Castings 15Cr - 4.6Ni - 0.22Cb - 2.8Cu Solution and Precipitation Heat Treated (H1100) 130 ksi (896 MPa) Tensile Strength
  • 2016 SAE AMS5356D-2016 Steel@ Corrosion Resistant@ Investment Castings 15Cr - 4.6Ni - 0.22Cb - 2.8Cu Solution and Precipitation Heat Treated (H1100) 130 ksi (896 MPa) Tensile Strength (UNS J92110)
  • 2011 SAE AMS5356-2011 STEEL CASTINGS, INVESTMENT, CORROSION RESISTANT 15Cr - 4.6Ni - 0.22(Cb + Ta) - 2.8Cu Solution and Precipitation Heat Treated 130,000 psi (696 MPa) Tensile Strength
  • 2010 SAE AMS5356C-2010 Steel, Corrosion Resistant, Investment Castings 15Cr 4.6Ni 0.22Cb 2.8Cu Solution and Precipitation Heat Treated (H1100) 130 ksi (896 MPa) Tensile Strength
  • 2006 SAE AMS5356B-2006 Steel, Corrosion Resistant, Investment Castings 15Cr - 4.6Ni - 0.22Cb - 2.8Cu Solution and Precipitation Heat Treated (H1100) 130 ksi (896 MPa) Tensile Strength
  • 2001 SAE AMS5356B-2001 Steel, Corrosion Resistant, Investment Castings 15Cr 4.6Ni 0.22Cb 2.8Cu Solution and Precipitation Heat Treated (H1100) 130 ksi (896 MPa) Tensile Strength
  • 1995 SAE AMS5356A-1995 Steel, Corrosion Resistant, Investment Castings 15Cr 4.6Ni 0.22Cb 2.8Cu Solution and Precipitation Heat Treated (H1100) 130 ksi (896 MPa) Tensile Strength