SAE AMS5398B-1978
STEEL CASTINGS, SAND AND CENTRIFUGAL, CORROSION RESISTANT 16Cr - 4.1Ni - 0.22(Cb+Ta) - 2.8Cu

Standard No.
SAE AMS5398B-1978
Release Date
1978
Published By
Society of Automotive Engineers (SAE)
Status
 2012-12
Replace By
SAE AMS5398C-1985
Latest
SAE AMS5398H-2023
Scope
This specification covers a corrosion-resistant steel in the form of sand or centrifugal castings.

SAE AMS5398B-1978 history

  • 2023 SAE AMS5398H-2023 Steel, Corrosion-Resistant, Sand and Centrifugal Castings 16Cr - 4.1Ni - 0.22Cb (Nb) - 2.8Cu Solution Heat Treated
  • 2018 SAE AMS5398H-2018 Steel@ Corrosion-Resistant@ Sand and Centrifugal Castings 16Cr - 4.1Ni - 0.22Cb (Nb) - 2.8Cu Solution Heat Treated (UNS J92200)
  • 2011 SAE AMS5398G-2011 Steel, Corrosion Resistant, Sand and Centrifugal Castings 16Cr 4.1Ni 0.22Cb(Nb) 2.8Cu Solution Heat Treated
  • 2006 SAE AMS5398F-2006 Steel, Corrosion Resistant, Sand and Centrifugal Castings 16Cr - 4.1Ni - 0.22(Cb + Ta) - 2.8Cu Solution Heat Treated UNS J92200
  • 2000 SAE AMS5398E-2000 Steel, Corrosion Resistant, Sand and Centrifugal Castings 16Cr 4.1Ni 0.22(Cb + Ta) 2.8Cu Solution Heat Treated
  • 1995 SAE AMS5398D-1995 STEEL CASTINGS, SAND AND CENTRIFUGAL, CORROSION RESISTANT 16Cr - 4.1Ni - 0.22(Cb + Ta) - 2.8Cu Solution Heat Treated, Precipitation Hardenable
  • 1989 SAE AMS5398D-1989 Steel Castings@ Sand and Centrifugal@ Corrosion Resistant 16Cr - 4.1Ni - 0.22(Cb + Ta) - 2.8Cu Solution Heat Treated@ Precipitation Hardenable
  • 1985 SAE AMS5398C-1985 Steel Castings@ Sand and Centrifugal@ Corrosion Resistant 16Cr - 4.1Ni - 0.22(cb + Ta) - 2.8Cu Solution Heat Treated (UNS J92170)
  • 1978 SAE AMS5398B-1978 STEEL CASTINGS, SAND AND CENTRIFUGAL, CORROSION RESISTANT 16Cr - 4.1Ni - 0.22(Cb+Ta) - 2.8Cu
  • 1961 SAE AMS5398A-1961 Steel Castings@ Sand and Centrifugal@ Corrosion Resistant 16Cr - 4.1Ni - 0.22 - 2.8Cu
  • 1955 SAE AMS5398-1955 STEEL CASTINGS, SAND, CORROSION RESISTANT 17Cr - 4Ni - 4Cu