SAE AMS5671-1965
ALLOY FORGINGS AND RINGS, CORROSION AND HEAT RESISTANT Nickel Base - 15.5Cr - 0.95(Cb + Ta) - 2.5Ti - 0.70Al - 7.0Fe Consumable Electrode or Vacuum Induction Melted

Standard No.
SAE AMS5671-1965
Release Date
1965
Published By
Society of Automotive Engineers (SAE)
Status
Replace By
SAE AMS5671A-1968
Latest
SAE AMS5671H-2019

SAE AMS5671-1965 history

  • 2019 SAE AMS5671H-2019 Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 72Ni - 15.5Cr - 0.95Cb - 2.5Ti - 0.70Al - 7.0Fe Consumable Electrode or Vacuum Induction Melted 1800 °F (982 °C) Solution Heat Treated, Precipitation Hardenable
  • 2013 SAE AMS5671G-2013 Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 72Ni - 15.5Cr - 0.95Cb - 2.5Ti - 0.70Al - 7.0Fe Consumable Electrode or Vacuum Induction Melted 1800 °F (982 °C) Solution Heat Treated, Precipitation Hardenable
  • 2003 SAE AMS5671G-2003 Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 72Ni - 15.5Cr - 0.95Cb - 2.5Ti - 0.70Al - 7.0Fe Consumable Electrode or Vacuum Induction Melted 1800 °F (982 °C) Solution Heat Treated, Precipitation Hardenable UNS N07750
  • 1996 SAE AMS5671F-1996 Nickel Alloy@ Corrosion and Heat Resistant@ Bars@ Forgings@ and Rings 72Ni - 15.5Cr - 0.95Cb - 2.5Ti - 0.70Al - 7.0Fe Consumable Electrode or Vacuum Induction Melted 1800 Degrees F (982 Deg. C) Solution Heat Treated@ Precipitation Hardenable@ Specificatio
  • 1989 SAE AMS5671E-1989 ALLOY BARS, FORGINGS, AND RINGS, CORROSION AND HEAT RESISTANT 72Ni - 15.5Cr - 0.95(Cb + Ta) - 2.5Ti - 0.70Al - 7.0Fe Consumable Electrode or Vacuum Induction Melted 1800°F (982°C) Solution Heat Treated, Precipitation Hardenable
  • 1979 SAE AMS5671D-1979 ALLOY BARS, FORGINGS, AND RINGS, CORROSION AND HEAT RESISTANT 72Ni - 15.5Cr - 0.95(Cb + Ta) - 2.5Ti - 0.70Al - 7.0Fe Consumable Electrode or Vacuum Induction Melted 1800° F (982° C) Solution Heat Treated
  • 1978 SAE AMS5671C-1978 ALLOY BARS, FORGINGS, AND RINGS, CORROSION AND HEAT RESISTANT 72Ni - 15.5Cr - 0.95(Cb + Ta) - 2.5Ti - 0.70Al - 7.0Fe Consumable Electrode or Vacuum Induction Melted 1800° F (982° C) Solution Heat Treated
  • 1969 SAE AMS5671B-1969 ALLOY BARS, FORGINGS, AND RINGS, CORROSION AND HEAT RESISTANT Nickel Base - 15.5Cr - 0.95(Cb + Ta) - 2.5Ti - 0.70Al - 7.0Fe Consumable Electrode or Vacuum Induction Melted
  • 1968 SAE AMS5671A-1968 ALLOY BARS, FORGINGS, AND RINGS, CORROSION AND HEAT RESISTANT Nickel Base - 15.5Cr - 0.95(Cb + Ta) - 2.5Ti - 0.70Al - 7.0Fe Consumable Electrode or Vacuum Induction Melted
  • 1965 SAE AMS5671-1965 ALLOY FORGINGS AND RINGS, CORROSION AND HEAT RESISTANT Nickel Base - 15.5Cr - 0.95(Cb + Ta) - 2.5Ti - 0.70Al - 7.0Fe Consumable Electrode or Vacuum Induction Melted