ALLOY BARS, FORGINGS, AND RINGS, CORROSION AND HEAT RESISTANT Nickel Base - 15.5Cr - 0.95(Cb + Ta) - 2.5Ti - 0.70Al - 7.0Fe Consumable Electrode or Vacuum Induction Melted
Home
SAE AMS5671A-1968
Standard No.
SAE AMS5671A-1968
Release Date
1968
Published By
Society of Automotive Engineers (SAE)
Status
Be replaced
Replace By
SAE AMS5671B-1969
Latest
SAE AMS5671H-2019
SAE AMS5671A-1968 history
2019
SAE AMS5671H-2019
Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 72Ni - 15.5Cr - 0.95Cb - 2.5Ti - 0.70Al - 7.0Fe Consumable Electrode or Vacuum Induction Melted 1800 °F (982 °C) Solution Heat Treated, Precipitation Hardenable
2013
SAE AMS5671G-2013
Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 72Ni - 15.5Cr - 0.95Cb - 2.5Ti - 0.70Al - 7.0Fe Consumable Electrode or Vacuum Induction Melted 1800 °F (982 °C) Solution Heat Treated, Precipitation Hardenable
2003
SAE AMS5671G-2003
Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 72Ni - 15.5Cr - 0.95Cb - 2.5Ti - 0.70Al - 7.0Fe Consumable Electrode or Vacuum Induction Melted 1800 °F (982 °C) Solution Heat Treated, Precipitation Hardenable UNS N07750
1996
SAE AMS5671F-1996
Nickel Alloy@ Corrosion and Heat Resistant@ Bars@ Forgings@ and Rings 72Ni - 15.5Cr - 0.95Cb - 2.5Ti - 0.70Al - 7.0Fe Consumable Electrode or Vacuum Induction Melted 1800 Degrees F (982 Deg. C) Solution Heat Treated@ Precipitation Hardenable@ Specificatio
1989
SAE AMS5671E-1989
ALLOY BARS, FORGINGS, AND RINGS, CORROSION AND HEAT RESISTANT 72Ni - 15.5Cr - 0.95(Cb + Ta) - 2.5Ti - 0.70Al - 7.0Fe Consumable Electrode or Vacuum Induction Melted 1800°F (982°C) Solution Heat Treated, Precipitation Hardenable
1979
SAE AMS5671D-1979
ALLOY BARS, FORGINGS, AND RINGS, CORROSION AND HEAT RESISTANT 72Ni - 15.5Cr - 0.95(Cb + Ta) - 2.5Ti - 0.70Al - 7.0Fe Consumable Electrode or Vacuum Induction Melted 1800° F (982° C) Solution Heat Treated
1978
SAE AMS5671C-1978
ALLOY BARS, FORGINGS, AND RINGS, CORROSION AND HEAT RESISTANT 72Ni - 15.5Cr - 0.95(Cb + Ta) - 2.5Ti - 0.70Al - 7.0Fe Consumable Electrode or Vacuum Induction Melted 1800° F (982° C) Solution Heat Treated
1969
SAE AMS5671B-1969
ALLOY BARS, FORGINGS, AND RINGS, CORROSION AND HEAT RESISTANT Nickel Base - 15.5Cr - 0.95(Cb + Ta) - 2.5Ti - 0.70Al - 7.0Fe Consumable Electrode or Vacuum Induction Melted
1968
SAE AMS5671A-1968
ALLOY BARS, FORGINGS, AND RINGS, CORROSION AND HEAT RESISTANT Nickel Base - 15.5Cr - 0.95(Cb + Ta) - 2.5Ti - 0.70Al - 7.0Fe Consumable Electrode or Vacuum Induction Melted
1965
SAE AMS5671-1965
ALLOY FORGINGS AND RINGS, CORROSION AND HEAT RESISTANT Nickel Base - 15.5Cr - 0.95(Cb + Ta) - 2.5Ti - 0.70Al - 7.0Fe Consumable Electrode or Vacuum Induction Melted
Copyright ©2023 All Rights Reserved