Scope
This document specifies the procedure and requirements for heat treating Nitralloy 135M, Nitralloy EZ, Nitralloy N, 4140, 4340, and H11 steels and for the subsequent gas nitriding of these alloys by the use of raw or dissociated ammonia.

SAE AMS2759/6-1992 history

  • 2018 SAE AMS2759/6C-2018 Gas Nitriding and Heat Treatment of Low-Alloy Steel Parts [Superseded: SAE AMS-S-6090B, SAE AMS-S-6090A, SAE AMS-S-6090]
  • 2014 SAE AMS2759/6B-2014 Gas Nitriding and Heat Treatment of Low-Alloy Steel Parts
  • 2005 SAE AMS2759/6B-2005 Gas Nitriding and Heat Treatment of Low-Alloy Steel Parts [Superseded: SAE AMS-S-6090B, SAE AMS-S-6090A, SAE AMS-S-6090]
  • 2002 SAE AMS2759/6A-2002 Gas Nitriding and Heat Treatment of Low-Alloy Steel Parts
  • 1992 SAE AMS2759/6-1992 GAS NITRIDING AND HEAT TREATMENT OF LOW-ALLOY STEEL PARTS
  • 1987 SAE AMS2759/6-1987 Gas Nitriding and Heat Treatment of Low-Alloy Steel Parts

SAE AMS2759/6-1992 -All Parts

SAE AMS2759-1984 HEAT TREATMENT OF STEEL PARTS General Requirements SAE AMS2759/1-1994 Heat Treatment of Carbon and Low-Alloy Steel Parts, Minimum Tensile Strength Below 220 ksi (1517 MPa) SAE AMS2759/10-1999 Automated Gaseous Nitriding Controlled by Nitriding Potential SAE AMS2759/10A-2014 Automated Gaseous Nitriding Controlled by Nitriding Potential SAE AMS2759/10B-2018 Automated Gaseous Nitriding Controlled by Nitriding Potential SAE AMS2759/11-2014 Stress Relief of Steel Parts SAE AMS2759/11A-2018 Stress Relief of Steel Parts SAE AMS2759/12-2007 Gaseous Nitrocarburizing@ Automatically Controlled by Potentials SAE AMS2759/12A-2007 Gaseous Nitrocarburizing, Automatically Controlled by Potentials SAE AMS2759/12B-2018 Gaseous Nitrocarburizing, Automatically Controlled by Potentials SAE AMS2759/13-2018 Gaseous Nitrocarburizing SAE AMS2759/1A-1996 Heat Treatment of Carbon and Low-Alloy Steel Parts Minimum Tensile Strength Below 220 ksi (1517 MPa) SAE AMS2759/1B-1996 Heat Treatment of Carbon and Low-Alloy Steel Parts Minimum Tensile Strength Below 220 ksi (1517 MPa) SAE AMS2759/1C-2000 Heat Treatment of Carbon and Low-Alloy Steel Parts Minimum Tensile Strength Below 220 ksi (1517 MPa) SAE AMS2759/1D-2007 Heat Treatment of Carbon and Low-Alloy Steel Parts Minimum Tensile Strength Below 220 ksi (1517 MPa) SAE AMS2759/1E-2014 Heat Treatement of Carbon and Low-Alloy Steel Parts Minimum Tensile Strength Below 220 ksi (1517 MPa) SAE AMS2759/1F-2018 Heat Treatment of Carbon and Low-Alloy Steel Parts Minimum Tensile Strength Below 220 ksi (1517 MPa) SAE AMS2759/1G-2019 Heat Treatment of Carbon and Low-Alloy Steel Parts Minimum Tensile Strength Below 220 ksi (1517 MPa) SAE AMS2759/1H-2019 Heat Treatment of Carbon and Low-Alloy Steel Parts Minimum Tensile Strength Below 220 ksi (1517 MPa) SAE AMS2759/1J-2021 Heat Treatment of Carbon and Low-Alloy Steel Parts Minimum Tensile Strength Below 220 ksi (1517 MPa) SAE AMS2759/2-2011 Heat Treatment of Low-Alloy Steel Parts Minimum Tensile Strength 220 ksi (1517 MPa) and Higher SAE AMS2759/2A-1996 Heat Treatment of Low-Alloy Steel Parts Minimum Tensile Strength 220 ksi (1517 MPa) and Higher SAE AMS2759/2B-1996 Heat Treatment of Low-Alloy Steel Parts Minimum Tensile Strength 220 ksi (1517 MPa) and Higher SAE AMS2759/2C-2000 Heat Treatment of Low-Alloy Steel Parts Minimum Tensile Strength 220 Ksi (1517 MPa) and Higher SAE AMS2759/2D-2007 Heat Treatment of Low-Alloy Steel Parts Minimum Tensile Strength 220 ksi (1517 MPa) and Higher SAE AMS2759/2E-2009 Heat Treatment of Low-Alloy Steel Parts Minimum Tensile Strength 220 ksi (1517 MPa) and Higher SAE AMS2759/2F-2014 Heat Treatment of Low-Alloy Steel Parts Minimum Tensile Strength 220 ksi (1517 MPa) and Higher SAE AMS2759/2G-2018 Heat Treatment of Low-Alloy Steel Parts Minimum Tensile Strength 220 ksi (1517 MPa) and Higher SAE AMS2759/2H-2018 Heat Treatment of Low-Alloy Steel Parts Minimum Tensile Strength 220 ksi (1517 MPa) and Higher SAE AMS2759/2J-2019 Heat Treatment of Low-Alloy Steel Parts Minimum Tensile Strength 220 ksi (1517 MPa) and Higher SAE AMS2759/2K-2021 Heat Treatment of Low-Alloy Steel Parts Minimum Tensile Strength 220 ksi (1517 MPa) and Higher SAE AMS2759/3-2011 Heat Treatment, Precipitation-Hardening Corrosion-Resistant and Maraging Steel Parts SAE AMS2759/3A-1996 Heat Treatment Precipitation-Hardening Corrosion-Resistant and Maraging Steel Parts SAE AMS2759/3B-1996 Heat Treatment Precipitation-Hardening Corrosion-Resistant and Maraging Steel Parts SAE AMS2759/3C-2000 Heat Treatment Precipitation-Hardening Corrosion-Resistant and Maraging Steel Parts SAE AMS2759/3D-2005 Heat Treatment Precipitation-Hardening Corrosion-Resistant and Maraging Steel Parts SAE AMS2759/3E-2014 Heat Treatment Precipitation-Hardening Corrosion-Resistant and Maraging Steel parts SAE AMS2759/3F-2015 Heat Treatment Precipitation-Hardening Corrosion-Resistant and Maraging Steel Parts SAE AMS2759/3G-2018 Heat Treatment Precipitation-Hardening Corrosion-Resistant and Maraging Steel Parts SAE AMS2759/3H-2019 Heat Treatment Precipitation-Hardening Corrosion-Resistant, Maraging, and Secondary Hardening Steel Parts SAE AMS2759/3J-2020 Heat Treatment Precipitation-Hardening Corrosion-Resistant, Maraging, and Secondary Hardening Steel Parts SAE AMS2759/4-2011 Heat Treatment, Austenitic Corrosion-Resistant Steel Parts SAE AMS2759/4A-1996 HEAT TREATMENT AUSTENITIC CORROSION-RESISTANT STEEL PARTS



Copyright ©2024 All Rights Reserved