This specification covers a corrosion and heat resistant nickel-base alloy in the form of bars, forgings, flash welded rings, and stock for forging and flash welded rings.
SAE AMS5703-1971 history
2023SAE AMS5703F-2023 Nickel Alloy, Corrosion- and Heat-Resistant, Bars, Forgings, and Rings and Stock for Forging 41.5Ni - 16Cr - 37Fe - 2.9Cb - 1.8Ti Consumable Electrode or Vacuum Induction Melted 1750 °F (954 °C) Solution, Stabilization, and Precipitation Heat Treated
2018SAE AMS5703E-2018 Nickel Alloy@ Corrosion and Heat-Resistant@ Bars@ Forgings@ and Rings 41.5Ni - 16Cr - 37Fe - 2.9Cb - 1.8Ti Consumable Electrode or Vacuum Induction Melted 1750 °F (954 °C) Solution@ Stabilization@ and Precipitation Heat Treated (UNS N09706)
2012SAE AMS5703D-2012 Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 41.5Ni - 16Cr - 37Fe - 2.9Cb - 1.8Ti Consumable Electrode or Vacuum Induction Melted 1750 °F (954 °C) Solution, Stabilization, and Precipitation Heat Treated
2006SAE AMS5703D-2006 Nickel Alloy, Corrosion and Heat Resistant, Bars, Forgings, and Rings 41.5Ni - 16Cr - 37Fe - 2.9Cb - 1.8Ti Consumable Electrode or Vacuum Induction Melted 1750 Degrees F (954 Degrees C) Solution, Stabilization, and Precipitation Heat Treated UNS N09706
2000SAE AMS5703C-2000 Nickel Alloy, Corrosion and Heat Resistant, Bars, Forgings, and Rings 41.5Ni - 16Cr - 37Fe - 2.9Cb - 1.8Ti Consumable Electrode or Vacuum Induction Melted 1750 °F (954 °C) Solution, Stabilization, and Precipitation Heat Treated
1993SAE AMS5703C-1993 Nickel Alloy, Corrosion and Heat Resistant, Bars, Forgings, and Rings 41.5Ni 16Cr 37Fe 2.9Cb 1.8Ti, Consumable Electrode or Vacuum Induction Melted, 1750°F (954°C) Solution, Stabilization, and Precipitation Heat Treated
1988SAE AMS5703B-1988 ALLOY BARS, FORGINGS, AND RINGS CORROSION AND HEAT RESISTANT 41.5Ni - 16Cr - 37Fe - 2.9Cb - 1.8Ti Consumable Electrode or Vacuum Induction Melted, 1750°F (955°C) Solution, Stabilization, and Precipitation Heat Treated
1981SAE AMS5703A-1981 ALLOY BARS, FORGINGS, AND RINGS, CORROSION AND HEAT RESISTANT 41.5Ni - 16Cr - 37Fe - 2.9Cb - 1.8Ti Consumable Electrode or Vacuum Induction Melted, 1750°F (955°C) Solution, Stabilization, and Precipitation Heat Treated
1971SAE AMS5703-1971 ALLOY BARS, FORGINGS, AND RINGS, CORROSION AND HEAT RESISTANT Nickel Base - 16Cr - 37Fe - 2.9Cb - 1.8Ti Consumable Electrode or Vacuum Induction Melted, 1750 F (954.4 C) Solution, Stabilization, and Precipitation Heat Treated