SAE AMS4439D-1992
Magnesium Alloy Castings@ Sand 4.2Zn - 1.2Ce - 0.7Zr (ZE41A-T5) Precipitation Heat Treated

Standard No.
SAE AMS4439D-1992
Release Date
1992
Published By
SAE - SAE International
Status
Replace By
SAE AMS4439D-2000
Latest
SAE AMS4439H-2018

SAE AMS4439D-1992 history

  • 1970 SAE AMS4439H-2018 Magnesium Alloy Castings 4.2Zn - 1.2Rare Earths - 0.7Zr (ZE41A-T5) Precipitation Heat Treated UNS M16410
  • 2012 SAE AMS4439G-2012 Magnesium Alloy Castings 4.2Zn 1.2 Rare Earths - O.7Zr (ZE41A-T5) Precipitation Heat Treated
  • 2007 SAE AMS4439F-2007 Magnesium Alloy Castings 4.2Zn - 1.2Rare Earths - 0.7Zr (ZE41A-T5) Precipitation Heat Treated UNS M16410
  • 2001 SAE AMS4439E-2001 Magnesium Alloy Castings 4.2Zn 1.2Ce O.70Zr (ZE41A-T5) Precipitation Heat Treated
  • 2000 SAE AMS4439D-2000 MAGNESIUM ALLOY CASTINGS, SAND 4.2Zn - 1.2Ce - 0.7Zr (ZE41A-T5) Precipitation Heat Treated
  • 1992 SAE AMS4439D-1992 Magnesium Alloy Castings@ Sand 4.2Zn - 1.2Ce - 0.7Zr (ZE41A-T5) Precipitation Heat Treated
  • 1985 SAE AMS4439C-1985 MAGNESIUM ALLOY CASTINGS@ SAND 4.2Zn - 1.2Ce - 0.70Zr (ZE41A-T5) Precipitation Heat Treated (UNS M16410)
  • 1979 SAE AMS4439B-1979 MAGNESIUM ALLOY CASTINGS@ SAND 4.2Zn - 1.2Ce - 0.7Zr (ZE41A-T5) Precipitation Heat Treated (UNS M16410)
  • 1976 SAE AMS4439A-1976 MAGNESIUM ALLOY CASTINGS@ SAND 4.2Zn - 1.2Ce - 0.7Zr (ZE41A-T5) Precipitation Heat Treated
  • 1970 SAE AMS4439-1970 MAGNESIUM ALLOY CASTINGS@ SAND 4.2Zn - 1.2Ce - 0.7Zr (ZE41A-T5) Precipitation Heat Treated