Scope

1.1 This specification2 covers austenitic alloy steel pipe for use in high-temperature, corrosive, or nuclear pressure service.

1.2 Several grades of austenitic stainless steel are covered as indicated in Table 1.

(A) Where ellipses (...) appear in this table there is no requirement, and the element need not be analyzed or reported.
(B) Grades CPF10MC and CPF8C may have a columbium plus tantalum content maximum of 1.358201;%.
(C) No designation as yet assigned by ASTM International or Steel Founders' Society of America.
(D) By agreement between the manufacturer and the purchaser, the carbon content of Grade CPH20 may be restricted to 0.108201;% max. When so agreed, the grade designation shall be CPH10.

1.3 Optional supplementary requirements are provided when additional testing may be required.

1.4 The values stated in either SI units or inch-pound units are to be regarded separately as standard. The values stated in each system may not be exact equivalents; therefore, each system shall be used independently of the other. Combining values from the two systems may result in non-conformance with the standard.

Note 1: This specification is not intended to cover centrifugal pipe made from alloys containing more than 0.208201;% carbon, such as are covered by Specification A297/A297M.

1.4.1 Within the text, the SI units are shown in brackets.

ASTM A451/A451M-14 Referenced Document

  • ASTM A297/A297M Standard Specification for Steel Castings, Iron-Chromium and Iron-Chromium-Nickel, Heat Resistant, for General Application
  • ASTM A999/A999M Standard Specification for General Requirements for Alloy and Stainless Steel Pipe
  • ASTM E165 Standard Test Method for Liquid Penetrant Examination
  • ASTM E186 Standard Reference Radiographs for Heavy-Walled (2 to 4 &189; in. [51 to 114-mm]) Steel Castings
  • ASTM E280 Standard Reference Radiographs for Heavy-Walled (4 &189; to 12-in. [114 to 305-mm]) Steel Castings
  • ASTM E29 Standard Practice for Using Significant Digits in Test Data to Determine Conformance with Specifications
  • ASTM E446 Standard Reference Radiographs for Steel Castings Up to 2 in. [51 mm] in Thickness
  • ASTM E94 Standard Guide for Radiographic Examination

ASTM A451/A451M-14 history

  • 2020 ASTM A451/A451M-20 Standard Specification for Centrifugally Cast Austenitic Steel Pipe for High-Temperature Service
  • 2019 ASTM A451/A451M-19 Standard Specification for Centrifugally Cast Austenitic Steel Pipe for High-Temperature Service
  • 2014 ASTM A451/A451M-14 Standard Specification for Centrifugally Cast Austenitic Steel Pipe for High-Temperature Service
  • 2006 ASTM A451/A451M-06(2010) Standard Specification for Centrifugally Cast Austenitic Steel Pipe for High-Temperature Service
  • 2006 ASTM A451/A451M-06 Standard Specification for Centrifugally Cast Austenitic Steel Pipe for High-Temperature Service
  • 2002 ASTM A451/A451M-02 Standard Specification for Centrifugally Cast Austenitic Steel Pipe for High-Temperature Service
  • 1993 ASTM A451-93(2002) Standard Specification for Centrifugally Cast Austenitic Steel Pipe for High-Temperature Service
  • 1993 ASTM A451-93(1997) Standard Specification for Centrifugally Cast Austenitic Steel Pipe for High-Temperature Service
Standard Specification for  Centrifugally Cast Austenitic Steel Pipe for High-Temperature   Service



Copyright ©2024 All Rights Reserved