SAE AMS5919A-2013
Cobalt-Nickel Alloy, Corrosion and Heat-Resistant, Round Bars 19Cr 36Co 25Ni 7.0Mo 0.50Cb (Nb) 2.9Ti 0.20Al 9.0Fe Vacuum Induction Plus Vacuum Consumable Electrode Melted Solution Heat Treated and Work Strengthened, Modificed Strength

Standard No.
SAE AMS5919A-2013
Release Date
2013
Published By
Society of Automotive Engineers (SAE)
Status
 2018-08
Replace By
SAE AMS5919B-2018
Latest
SAE AMS5919B-2018
Scope
This specification covers a corrosion and heat-resistant, work strengthened cobalt-nickel-chromium alloy in the form of bars 2 inches (50.8 mm) and under in nominal diameter. These bars have been used typically for parts, such as fasteners, requiring a room temperature minimum tensile strength of 170 ksi (1172 MPa) for use up to 850 °F (454 °C) in applications requiring high ductility to promote toughness and resistance to cracking under shock loading conditions, but usage is not limited to such applications. This alloy exhibits exceptionally good resistance to corrosion, crevice corrosion, and stress-corrosion cracking.

SAE AMS5919A-2013 Referenced Document

  • ASTM E112-12 Standard Test Methods for Determining Average Grain Size*2024-04-20 Update
  • ASTM E18-11 Standard Test Methods for Rockwell Hardness of Metallic Materials*2024-04-20 Update
  • ASTM E8-04 Standard Test Methods for Tension Testing of Metallic Materials*2024-04-20 Update
  • ASTM E8M-04 Standard Test Methods for Tension Testing of Metallic Materials [Metric] *2024-04-20 Update
  • SAE AMS2261 TOLERANCES Nickel and Nickel Base Alloy Bars
  • SAE AMS2269 CHEMICAL CHECK ANALYSIS LIMITS Wrought Nickel and Nickel Base Alloys
  • SAE AMS2371 QUALITY ASSURANCE SAMPLING OF CORROSION AND HEAT RESISTANT ALLOYS Wrought Products and Forging Stock
  • SAE AMS2750 PYROMETRY
  • SAE AMS2806 IDENTIFICATION Bars, Wire, Mechanical Tubing, and Extrusions Carbon and Alloy Steels and Heat and Corrosion Resistant Steels and Alloys

SAE AMS5919A-2013 history

  • 2018 SAE AMS5919B-2018 Cobalt-Nickel Alloy@ Corrosion and Heat-Resistant@ Round Bars 19Cr - 36Co - 25Ni - 7.0Mo - 0.50Cb (Nb) - 2.9Ti - 0.20Al - 9.0Fe Vacuum Induction Plus Vacuum Consumable Electrode Melted Solution Heat Treated and Work Strengthened@ Modified Strength (UNS R3
  • 2013 SAE AMS5919A-2013 Cobalt-Nickel Alloy, Corrosion and Heat-Resistant, Round Bars 19Cr 36Co 25Ni 7.0Mo 0.50Cb (Nb) 2.9Ti 0.20Al 9.0Fe Vacuum Induction Plus Vacuum Consumable Electrode Melted Solution Heat Treated and Work Strengthened, Modificed Strength
  • 2007 SAE AMS5919-2007 Cobalt-Nickel Alloy, Corrosion and Heat-Resistant, Round Bars 19Cr - 36Co - 25Ni - 7.0Mo - 0.50Cb - 2.9Ti - 0.20Al - 9.0Fe Vacuum Induction Plus Vacuum Consumable Electrode Melted Solution Heat Treated and Work Strengthened, Modified Strength
  • 2003 SAE AMS5919-2003 Cobalt-Nickel Alloy, Corrosion and Heat-Resistant, Round Bars 19Cr - 36Co - 25Ni - 7.0Mo - 0.50Cb - 2.9Ti - 0.20Al - 9.0Fe Vacuum Induction Plus Vacuum Consumable Electrode Melted Solution Heat Treated and Work Strengthened, Modified Strength UNS R30159