SAE AMS5354F-2012
Steel, Corrosion and Heat Resistant, Investment Castings 13Cr 2.0Ni 3.0W Hardened and Tempered to 32 - 38 HRC

Standard No.
SAE AMS5354F-2012
Release Date
2012
Published By
Society of Automotive Engineers (SAE)
Status
 2018-08
Replace By
SAE AMS5354G-2018
Latest
SAE AMS5354G-2023
Scope
This specification covers a corrosion and moderate heat resistant steel in the form of investment castings. These castings have been used typically for parts, such as compressor blades and vanes, housings, and valves, for use up to 1000 degrees F (538 degrees C), but usage is not limited to such applications.

SAE AMS5354F-2012 Referenced Document

  • ASTM E1417-05 Standard Practice for Liquid Penetrant Testing*2024-04-20 Update
  • ASTM E1444-05 Standard Practice for Magnetic Particle Testing*2024-04-20 Update
  • ASTM E1742-08 Standard Practice for Radiographic Examination*2024-04-20 Update
  • ASTM E18-11 Standard Test Methods for Rockwell Hardness of Metallic Materials*2024-04-20 Update
  • ASTM E8-04 Standard Test Methods for Tension Testing of Metallic Materials*2024-04-20 Update
  • ASTM E8M-04 Standard Test Methods for Tension Testing of Metallic Materials [Metric] *2024-04-20 Update
  • SAE AMS2175-2003 Castings, Classification and Inspection of
  • SAE AMS2248 CHEMICAL CHECK ANALYSIS LIMITS Wrought Heat and Corrosion Resistant Steels
  • SAE AMS2360 ROOM TEMPERATURE TENSILE PROPERTIES OF CASTINGS
  • SAE AMS2694 REPAIR WELDING OF AEROSPACE CASTINGS
  • SAE AMS2700-2000 Passivation of Corrosion Resistant Steels
  • SAE AMS2759 HEAT TREATMENT OF STEEL PARTS General Requirements
  • SAE AMS2759/5 Heat Treatment, Martensitic Corrosion-Resistant Steel Parts
  • SAE AMS2804 IDENTIFICATION Castings

SAE AMS5354F-2012 history

  • 2023 SAE AMS5354G-2023 Steel, Corrosion and Heat Resistant, Investment Castings 13Cr - 2.0Ni - 3.0W Hardened and Tempered to 32 - 38 HRC
  • 2018 SAE AMS5354G-2018 Steel@ Corrosion and Heat Resistant@ Investment Castings 13Cr - 2.0Ni - 3.0W Hardened and Tempered to 32 - 38 HRC (UNS J91631)
  • 2012 SAE AMS5354F-2012 Steel, Corrosion and Heat Resistant, Investment Castings 13Cr 2.0Ni 3.0W Hardened and Tempered to 32 - 38 HRC
  • 2006 SAE AMS5354E-2006 Steel, Corrosion and Heat Resistant, Investment Castings 13Cr - 2.0Ni - 3.0W Hardened and Tempered
  • 2001 SAE AMS5354E-2001 STEEL CASTINGS, INVESTMENT, CORROSION RESISTANT 13Cr - 2Ni - 3W
  • 1995 SAE AMS5354D-1995 STEEL CASTINGS, INVESTMENT, CORROSION AND MODERATE HEAT RESISTANT 13Cr - 2.0Ni - 3.0W Hardened and Tempered
  • 1982 SAE AMS5354D-1982 Steel Castings@ Investment@ Corrosion and Moderate Heat Resistant 13Cr - 2.0Ni - 3.0W Hardened and Tempered (UNS J91631)
  • 1975 SAE AMS5354C-1975 STEEL CASTINGS, INVESTMENT, CORROSION AND MODERATE HEAT RESISTANT 13Cr - 2Ni - 3W
  • 1962 SAE AMS5354B-1962 STEEL CASTINGS, INVESTMENT, CORROSION RESISTANT 13Cr - 2Ni - 3W
  • 1959 SAE AMS5354A-1959 STEEL CASTINGS, INVESTMENT, CORROSION RESISTANT 13Cr - 2Ni - 3W
  • 1947 SAE AMS5354-1947 STEEL CASTINGS, PRECISION INVESTMENT, CORROSION RESISTANT 13Cr - 3W - 2Ni



Copyright ©2024 All Rights Reserved