SAE AMS5402C-2004
Nickel Alloy, Corrosion and Heat Resistant, Investment Castings 62Ni 21.5Cr 9.0Mo 3.6Cb (Nb) As Cast

Standard No.
SAE AMS5402C-2004
Release Date
2004
Published By
Society of Automotive Engineers (SAE)
Status
Replace By
SAE AMS5402A-2011
Latest
SAE AMS5402D-2023
Scope
This specification covers a corrosion and heat resistant, air-melted, nickel alloy in the form of investment castings. These castings have been used typically for structural parts requiring strength up to 1200 degrees F (649 degrees C) and oxidation and corrosion resistance up to 1800 degrees F (982 degrees C), but usage is not limited to such applications.

SAE AMS5402C-2004 Referenced Document

SAE AMS5402C-2004 history

  • 2023 SAE AMS5402D-2023 Nickel Alloy, Corrosion- and Heat-Resistant, Investment Castings 62Ni - 21.5Cr - 9.0Mo - 3.6Cb (Nb) As Cast
  • 2018 SAE AMS5402D-2018 Nickel Alloy@ Corrosion and Heat-Resistant@ Investment Castings 62Ni - 21.5Cr - 9.0Mo - 3.6Cb (Nb) As Cast (UNS N26010)
  • 2011 SAE AMS5402C-2011 Nickel Alloy, Corrosion and Heat-Resistant, Investment Castings 62Ni - 21.5Cr - 9.0Mo - 3.6Cb (Nb) As Cast
  • 2011 SAE AMS5402A-2011 ALLOY CASTINGS, INVESTMENT, CORROSION AND HEAT RESISTANT 62Ni - 21.5Cr - 9.0Mo - 3.6(Cb+Ta) As Cast
  • 2004 SAE AMS5402C-2004 Nickel Alloy, Corrosion and Heat Resistant, Investment Castings 62Ni 21.5Cr 9.0Mo 3.6Cb (Nb) As Cast
  • 1996 SAE AMS5402B-1996 (R) Nickel Alloy, Corrosion and Heat Resistant, Investment Castings 62Ni - 21.5Cr - 9.0Mo - 3.6Cb as Cast (UNS N26625)
  • 1980 SAE AMS5402-1980 ALLOY CASTINGS, INVESTMENT, CORROSION AND HEAT RESISTANT 62Ni - 21.5Cr - 9.0Mo - 3.6(Cb+Ta)