This specification covers a corrosion and heat resistant steel in the form of seamless tubing. This turbine has been used typically for parts requiring both corrosion and heat resistance, especially when such parts are welded during fabrication, but usage is not limited to such applications. Also for parts requiring oxidation resistance up to 1500 °F (816 °C), but useful at that temperature only when stresses are low.
SAE AMS5571J-2012 Referenced Document
ASTM A262-10 Standard Practices for Detecting Susceptibility to Intergranular Attack in Austenitic Stainless Steels*, 2024-04-19 Update
ASTM A370-11 Standard Test Methods and Definitions for Mechanical Testing of Steel Products*, 2024-04-19 Update
ASTM E426-98 Standard Practice for Electromagnetic (Eddy-Current) Examination of Seamless and Welded Tubular Products, Austenitic Stainless Steel and Similar Alloys