SAE AMS4462-2011
Aluminum Alloy, Sheet and Plate, Alclad 4.4Cu 1.5Mg 0.60Mn (Alclad 2024, -T3 Sheet, -T351 Plate) Solution Heat Treated, Cold Worked and Naturally Aged

Standard No.
SAE AMS4462-2011
Release Date
2011
Published By
Society of Automotive Engineers (SAE)
Status
Replace By
SAE AMS4462A-2018
Latest
SAE AMS4462A-2018
Scope
This specification covers an aluminum alloy in the form of sheet and plate supplied in the ?T3/?T351 temper. These products have been used typically for medium strength parts requiring formability and maximum corrosion resistance and whose fabrication does not involve welding; but usage is not limited to such applications.

SAE AMS4462-2011 Referenced Document

  • ASTM B594-09 Standard Practice for Ultrasonic Inspection of Aluminum-Alloy Wrought Products for Aerospace Applications*2024-04-19 Update
  • ASTM B660-08 Standard Practices for Packaging/Packing of Aluminum and Magnesium Products*2024-04-19 Update
  • ASTM B666/B666M-08 Standard Practice for Identification Marking of Aluminum and Magnesium Products*2024-04-19 Update
  • SAE AMS2355 TENSILE TESTING OF WROUGHT ALUMINUM AND MAGNESIUM PRODUCTS Except Forgings
  • SAE AMS2772-1997 Heat Treatment of Aluminum Alloy Raw Materials (01 1997)
  • SAE AS1990-1990 Aluminum Alloy Tempers

SAE AMS4462-2011 history

  • 2018 SAE AMS4462A-2018 Aluminum Alloy, Sheet and Plate, Alclad 4.4Cu - 1.5Mg - 0.60Mn (Alclad 2024, -T3 Sheet, -T351 Plate) Solution Heat Treated, Cold Worked and Naturally Aged
  • 2011 SAE AMS4462-2011 Aluminum Alloy, Sheet and Plate, Alclad 4.4Cu 1.5Mg 0.60Mn (Alclad 2024, -T3 Sheet, -T351 Plate) Solution Heat Treated, Cold Worked and Naturally Aged



Copyright ©2024 All Rights Reserved