SAE AMS5441A-2011
Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings Ni 18Cr 2.8Mo 5.5Cb(Nb) 0.70Ti 1.50Al 10Fe 9Co 1W Consumable Electrode Remelted or Vacuum Induction Melted 1775 °F (968 °C) Solution Heat Treated, Precipitation-Hardenable

Standard No.
SAE AMS5441A-2011
Release Date
2011
Published By
Society of Automotive Engineers (SAE)
Status
 2016-11
Replace By
SAE AMS5441B-2016
Latest
SAE AMS5441C-2023
Scope
This specification covers a corrosion and heat-resistant nickel alloy in the form of bars, forgings, flash welded rings, and stock for forging, flash welded rings, or heading. These products have been used typically for parts requiring high resistance to creep and stress-rupture up to 1400 °F (760 °C) and oxidation resistance up to 1800 °F (982 °C), particularly those parts which are formed or welded and then precipitation heat treated to develop required properties, but usage is not limited to such applications.

SAE AMS5441A-2011 Referenced Document

  • ASTM E10-10 Standard Test Method for Brinell Hardness of Metallic Materials*2024-04-19 Update
  • ASTM E112-10 Standard Test Methods for Determining Average Grain Size*2024-04-19 Update
  • ASTM E139-11 Standard Test Methods for Conducting Creep, Creep-Rupture, and Stress-Rupture Tests of Metallic Materials*2024-04-19 Update
  • ASTM E21-09 Standard Test Methods for Elevated Temperature Tension Tests of Metallic Materials*2024-04-19 Update
  • ASTM E292-09 Standard Test Methods for Conducting Time-for-Rupture Notch Tension Tests of Materials*2024-04-19 Update
  • ASTM E8/E8M-09 Standard Test Methods for Tension Testing of Metallic Materials*2024-04-19 Update
  • SAE AMS2261 TOLERANCES Nickel and Nickel Base Alloy Bars
  • SAE AMS2269 CHEMICAL CHECK ANALYSIS LIMITS Wrought Nickel and Nickel Base Alloys
  • SAE AMS2371 QUALITY ASSURANCE SAMPLING OF CORROSION AND HEAT RESISTANT ALLOYS Wrought Products and Forging Stock
  • SAE AMS2374 QUALITY ASSURANCE SAMPLING OF CORROSION AND HEAT RESISTANT STEELS AND ALLOYS Forgings and Forging Stock
  • SAE AMS2750 PYROMETRY
  • SAE AMS2806 IDENTIFICATION Bars, Wire, Mechanical Tubing, and Extrusions Carbon and Alloy Steels and Heat and Corrosion Resistant Steels and Alloys
  • SAE AMS2808 IDENTIFICATION Forgings
  • SAE AMS7490 RINGS, FLASH WELDED Corrosion and Heat Resistant
  • SAE ARP1313 DETERMINATION OF TRACE ELEMENTS IN HIGH TEMPERATURE ALLOYS

SAE AMS5441A-2011 history

  • 1970 SAE AMS5441C-2023 Nickel Alloy, Corrosion- and Heat-Resistant, Bars, Forgings, and Rings Ni - 18Cr - 2.8Mo - 5.5Cb (Nb) - 0.70Ti - 1.50Al - 10Fe - 9Co - 1W Consumable Electrode Remelted or Vacuum Induction Melted 1775 °F (968 °C) Solution Heat Treated
  • 2016 SAE AMS5441B-2016 Nickel Alloy@ Corrosion and Heat-Resistant@ Bars@ Forgings@ and Rings Ni - 18Cr - 2.8Mo - 5.5Cb(Nb) - 0.70Ti - 1.50Al - 10Fe - 9Co - 1W Consumable Electrode Remelted or Vacuum Induction Melted 1775 °F (968 °C) Solution Heat Treated@ Precipitation-Hardenab
  • 2011 SAE AMS5441A-2011 Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings Ni 18Cr 2.8Mo 5.5Cb(Nb) 0.70Ti 1.50Al 10Fe 9Co 1W Consumable Electrode Remelted or Vacuum Induction Melted 1775 °F (968 °C) Solution Heat Treated, Precipitation-Hardenable
  • 2006 SAE AMS5441-2006 Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings Ni - 18Cr - 2.8Mo - 5.5Cb(Nb) - 0.70Ti - 1.50Al - 10Fe - 9Co - 1W Consumable Electrode Remelted or Vacuum Induction Melted 1775 degrees F (968 degrees C) Solution Heat Treated, Precipi



Copyright ©2024 All Rights Reserved