SAE AMS7911C-2010
Aluminum Beryllium, Preforms Hot Isostatic Pressed and Heat Treated 38Al 62Be

Standard No.
SAE AMS7911C-2010
Release Date
2010
Published By
Society of Automotive Engineers (SAE)
Status
Replace By
SAE AMS7911D-2015
Latest
SAE AMS7911E-2023
Scope
This specification covers aluminum and beryllium powders consolidated by hot isostatic pressing (HIP) into the form of bar, rod, tubing, and shapes. These performs have been used typically for parts requiring high thermal conductivity, low density, and high modulus of elasticity, but usage is not limited to such applications.

SAE AMS7911C-2010 history

  • 2023 SAE AMS7911E-2023 Aluminum Beryllium, Preforms Hot Isostatic Pressed and Heat Treated 38Al - 62Be
  • 2018 SAE AMS7911D-2018 Aluminum Beryllium, Preforms Hot Isostatic Pressed and Heat Treated 38Al - 62Be
  • 2015 SAE AMS7911D-2015 Aluminum Beryllium@ Preforms Hot Isostatic Pressed and Heat Treated 38Al - 62Be
  • 2010 SAE AMS7911C-2010 Aluminum Beryllium, Preforms Hot Isostatic Pressed and Heat Treated 38Al 62Be
  • 2005 SAE AMS7911B-2005 Aluminum Beryllium, Preforms Hot Isostatic Pressed 38Al - 62Be
  • 2001 SAE AMS7911A-2001 Aluminum Beryllium, Preforms Hot Isostatic Pressed 38Al - 62Be
  • 1995 SAE AMS7911-1995 Aluminum Beryllium@ Preforms Hot Isostatic Pressed 38Al - 62Be



Copyright ©2024 All Rights Reserved