SAE AMS-H-7199-1998
Heat Treatment of Wrought Copper-Beryllium Alloys, Process for (Copper Alloys: Numbers C17000, C17200, C17300, C17500, and C17510) [Superseded: NAVY MIL-H-7199 A CANC NOTICE 2, NAVY MIL-H-7199 A VALID NOTICE 1, NAVY MIL-H-7199 A (2), NAVY MIL-H-7199

Standard No.
SAE AMS-H-7199-1998
Release Date
1998
Published By
Society of Automotive Engineers (SAE)
Status
Replace By
SAE AMS-H-7199-2007
Latest
SAE AMS-H-7199A-2013
Scope
This specification presents requirements for the heat treatment of parts and components fabricated from wrought (plate, sheet, strip, bar, rod, wire extrusions and tube and forgings) copper alloys, numbers C17000, C17200, C17300, C17500, and C17510. This specification also covers bright hardening.

SAE AMS-H-7199-1998 history

  • 2013 SAE AMS-H-7199A-2013 Heat Treatment of Wrought Copper-Beryllium Alloys, Process for (Copper Alloys: Numbers C17000, C17200, C17300, C17500, and C17510)
  • 2007 SAE AMS-H-7199-2007 Heat Treatment of Wrought Copper-Beryllium Alloys, Process for (Copper Alloys: Numbers C17000, C17200, C17300, C17500, and C17510)
  • 1998 SAE AMS-H-7199-1998 Heat Treatment of Wrought Copper-Beryllium Alloys, Process for (Copper Alloys: Numbers C17000, C17200, C17300, C17500, and C17510) [Superseded: NAVY MIL-H-7199 A CANC NOTICE 2, NAVY MIL-H-7199 A VALID NOTICE 1, NAVY MIL-H-7199 A (2), NAVY MIL-H-7199



Copyright ©2024 All Rights Reserved