SAE AMS5588G-2010
Nickel Alloy, Corrosion and Heat Resistant, Welded Tubing 47.5Ni 22Cr 1.5Co 9.0Mo 0.60W 18.5Fe Solution Heat Treated

Standard No.
SAE AMS5588G-2010
Release Date
2010
Published By
Society of Automotive Engineers (SAE)
Status
Replace By
SAE AMS5588H-2022
Latest
SAE AMS5588H-2022
Scope
This specification covers a corrosion and heat resistant nickel alloy in the form of welded and drawn tubing. This tubing has been used typically for fluid lines operating in service under appreciable stresses at elevated temperatures, but usage is not limited to such applications. Alloy has good strength up to 1800 °F (982 °C) and oxidation resistance up to 2200 °F (1204 °C).

SAE AMS5588G-2010 Referenced Document

  • ASTM E112-10 Standard Test Methods for Determining Average Grain Size*2024-04-19 Update
  • ASTM E1417-05 Standard Practice for Liquid Penetrant Testing*2024-04-19 Update
  • ASTM E426-98 Standard Practice for Electromagnetic (Eddy-Current) Examination of Seamless and Welded Tubular Products, Austenitic Stainless Steel and Similar Alloys
  • ASTM E8-04 Standard Test Methods for Tension Testing of Metallic Materials*2024-04-19 Update
  • ASTM E8M-04 Standard Test Methods for Tension Testing of Metallic Materials [Metric] *2024-04-19 Update
  • SAE AMS2263E-2006 Tolerances Nickel, Nickel Alloy, and Cobalt Alloy Tubing [Superseded: SAE MAM 2263B, SAE MAM 2263A, SAE MAM 2263, SAE MAM 2263]
  • SAE AMS2269F-2006 Chemical Check Analysis Limits Nickel, Nickel Alloys, and Cobalt Alloys [Superseded: SAE AMS 2268B]
  • SAE AMS2371H-2007 Quality Assurance Sampling and Testing Corrosion and Heat-Resistant Steels and Alloys Wrought Products and Forging Stock*2024-04-19 Update
  • SAE AMS2632A-1995 Inspection, Ultrasonic, of Thin Materials 0.50 Inch (12.7mm) and under in Cross-Sectional Thickness
  • SAE AMS2807-1991 Identification Carbon and Low-Alloy Steels@ Corrosion and Heat Resistant Steels and Alloys Sheet@ Strip@ Plate@ and Aircraft Tubing

SAE AMS5588G-2010 history

  • 2022 SAE AMS5588H-2022 Nickel Alloy, Corrosion- and Heat-Resistant, Welded Tubing 47.5Ni - 22Cr - 1.5Co - 9.0Mo - 0.60W - 18.5Fe Solution Heat Treated
  • 2010 SAE AMS5588G-2010 Nickel Alloy, Corrosion and Heat Resistant, Welded Tubing 47.5Ni 22Cr 1.5Co 9.0Mo 0.60W 18.5Fe Solution Heat Treated
  • 2006 SAE AMS5588F-2006 Nickel Alloy, Corrosion and Heat Resistant, Welded Tubing 47.5Ni - 22Cr - 1.5Co - 9.0Mo - 0.60W - 18.5Fe Solution Heat Treated
  • 2000 SAE AMS5588F-2000 Nickel Alloy, Corrosion and Heat Resistant, Welded Tubing 47.5Ni 22Cr 1.5Co 9.0Mo 0.60W 18.5Fe Solution Heat Treated
  • 1995 SAE AMS5588E-1995 Nickel Alloy@ Corrosion and Heat Resistant@ Welded Tubing 47.5Ni - 22Cr - 1.5Co - 9.0Mo - 0.60W - 18.5Fe Solution Heat Treated (UNS N06002)
  • 1989 SAE AMS5588D-1989 ALLOY TUBING@ WELDED AND DRAWN@ CORROSION AND HEAT RESISTANT 47.5Ni - 22Cr - 1.5Co - 9.0Mo - 0.60W - 18.5Fe Solution Heat Treated (UNS N06002)
  • 1980 SAE AMS5588C-1980 ALLOY TUBING, WELDED AND DRAWN, CORROSION AND HEAT RESISTANT 47.5Ni - 22Cr - 1.5Co - 9.0Mo - 0.60W - 18.5Fe
  • 1968 SAE AMS5588B-1968 ALLOY TUBING, WELDED AND DRAWN, CORROSION AND HEAT RESISTANT Nickel Base - 22Cr - 1.5Co - 9.0Mo - 0.60W - 18.5Fe
  • 1966 SAE AMS5588A-1966 ALLOY TUBING, WELDED AND DRAWN, CORROSION AND HEAT RESISTANT Nickel Base - 22Cr - 1.5Co - 9.0Mo - 0.60W - 18.5Fe
  • 1965 SAE AMS5588-1965 ALLOY TUBING, WELDED AND DRAWN, CORROSION AND HEAT RESISTANT Nickel Base - 22Cr - 1.5Co - 9.0Mo - 0.60W - 18.5Fe



Copyright ©2024 All Rights Reserved