This part of EN 1071 describes a method of measuring the fracture strain of ceramic coatings by means of uniaxial tension or compression tests coupled with acoustic emission to monitor the onset of cracking of the coating. Tensile or compressive strains can also be applied by flexure using four-point bending. Measurements can be made in favourable cases at elevated temperatures as well as at room temperature.
EN 1071-9:2009 Referenced Document
EN 10002-1 Metallic Materials - Tensile Testing - Part 1: Method of Test at Ambient Temperature
EN 10002-5 Metallic Materials - Tensile Testing - Part 5: Method of Testing at Elevated Temperature
EN ISO/IEC 17025 General requirements for the competence of testing and calibration laboratories*, 2017-12-01 Update