SAE AMS5884C-2009
Iron-Nickel Alloy, Bars, Forgings, and Rings 42Fe 37.5Ni 14Co 4.8Cb(Nb) 1.6Ti Solution Heat Treated, Precipitation Hardenable Multiple Melted, High Temperature, Low Expansion

Standard No.
SAE AMS5884C-2009
Release Date
2009
Published By
Society of Automotive Engineers (SAE)
Status
 2016-01
Replace By
SAE AMS5884D-2016
Latest
SAE AMS5884E-2022
Scope
This specification covers an iron-nickel alloy in the form of bars, forgings, flash welded rings, and stock for forging, flash welded rings, or heading. These products have been used typically for parts requiring a combination of high strength and low expansion properties up to 1200 °F (649 °C), but usage is not limited to such applications.

SAE AMS5884C-2009 Referenced Document

  • ASTM E10-08 Standard Test Method for Brinell Hardness of Metallic Materials*2024-04-19 Update
  • ASTM E1181-02 Standard Test Methods for Characterizing Duplex Grain Sizes
  • ASTM E139-06 Standard Test Methods for Conducting Creep, Creep-Rupture, and Stress-Rupture Tests of Metallic Materials*2024-04-19 Update
  • ASTM E21-09 Standard Test Methods for Elevated Temperature Tension Tests of Metallic Materials*2024-04-19 Update
  • ASTM E228-06 Standard Test Method for Linear Thermal Expansion of Solid Materials With a Push-Rod Dilatometer*2024-04-19 Update
  • ASTM E292-09 Standard Test Methods for Conducting Time-for-Rupture Notch Tension Tests of Materials*2024-04-19 Update
  • ASTM E8/E8M-08 Standard Test Methods for Tension Testing of Metallic Materials*2024-04-19 Update
  • ASTM E8/E8M-09 Standard Test Methods for Tension Testing of Metallic Materials*2024-04-19 Update
  • ASTM E930-99 Standard Test Methods for Estimating the Largest Grain Observed in a Metallographic Section (ALA Grain Size)
  • SAE AMS2261 TOLERANCES Nickel and Nickel Base Alloy Bars
  • SAE AMS2261H-2007 Tolerances, Nickel, Nickel Alloy, and Cobalt Alloy, Bars, Rods, and Wire
  • SAE AMS2269F-2006 Chemical Check Analysis Limits Nickel, Nickel Alloys, and Cobalt Alloys [Superseded: SAE AMS 2268B]

SAE AMS5884C-2009 history

  • 2022 SAE AMS5884E-2022 Iron-Nickel Alloy, Bars, Forgings, and Rings 42Fe - 37.5Ni - 14Co - 4.8Cb (Nb) - 1.6Ti Solution Heat Treated, Precipitation Hardenable Multiple Melted, High Temperature, Low Expansion
  • 2016 SAE AMS5884D-2016 Iron-Nickel Alloy@ Bars@ Forgings@ and Rings 42Fe - 37.5Ni - 14Co - 4.8Cb(Nb) - 1.6Ti Solution Heat Treated@ Precipitation Hardenable Multiple Melted@ High Temperature@ Low Expansion (UNS N19909)
  • 2009 SAE AMS5884C-2009 Iron-Nickel Alloy, Bars, Forgings, and Rings 42Fe 37.5Ni 14Co 4.8Cb(Nb) 1.6Ti Solution Heat Treated, Precipitation Hardenable Multiple Melted, High Temperature, Low Expansion
  • 2006 SAE AMS5884B-2006 Iron-Nickel Alloy, Bars, Forgings, and Rings 42Fe - 37.5Ni - 14Co - 4.8Cb - 1.6Ti Solution Heat Treated, Precipitation Hardenable Multiple Melted, High Temperature, Low Expansion
  • 2001 SAE AMS5884B-2001 Iron-Nickel Alloy, Bars, Forgings, and Rings 42Fe 37.5Ni 14Co 4.8Cb 1.6Ti Solution Heat Treated, Precipitation Hardenable Multiple Melted, High Temperature, Low Expansion
  • 2000 SAE AMS5884A-2000 Iron-Nickel Alloy, Bars, Forgings, and Rings 42Fe - 37.5Ni - 14Co - 4.8Cb - 1.6Ti Solution Heat Treated, Precipitation Hardenable Multiple Melted, High Temperature, Low Expansion
  • 1994 SAE AMS5884A-1994 Iron-Nickel Alloy@ Bars@ Forgings@ and Rings 42Fe - 37.5Ni - 14Co - 4.8Cb - 1.6Ti Solution Heat Treated@ Precipitation Hardenable Multiple Melted@ High Temperature@ Low Expansion (UNS N19909)
  • 1992 SAE AMS5884-1992 IRON-NICKEL ALLOY, BARS, FORGINGS, AND RINGS 42Fe - 37.5Ni - 14Co - 4.8(Cb + Ta) - 1.6Ti Solution Heat Treated, Precipitation Hardenable Multiple Melted, High Temperature, Low Expansion



Copyright ©2024 All Rights Reserved