This European Standard describes two methods for determination of air content of compacted fresh concrete,
made with normal weight or relatively dense aggregate of maximum size up to 63 mm.
NOTE Neither method is applicable to concretes made with lightweight aggregates, air cooled blast-furnace slag, or
aggregates with high porosity, because of the magnitude of the aggregate correction factor, compared with the entrained
air content of the concrete.
BS EN 12350-7:2009 Referenced Document
EN 12350-1 Testing fresh concrete - Part 1: Sampling
EN 12350-6 Testing fresh concrete - Part 6: Density
BS EN 12350-7:2009 history
2019BS EN 12350-7:2019 Testing fresh concrete Part 7: Air content — Pressure methods
2009BS EN 12350-7:2009 Testing fresh concrete Part 7: Air content — Pressure methods
2000BS EN 12350-7:2000 Testing fresh concrete - Air content - Pressure methods