Scope

1.1 This specification covers UNS N08120, UNS N08800, UNS N08801, UNS N08810, UNS N08811, UNS N08890, and UNS N06811 in the form of cold-worked and hot-finished annealed seamless pipe and tube. Alloys UNS N08800 and UNS N06811 are normally employed in service temperatures up to and including 1100°F (593°C). Alloys UNS N08120, UNS N08810, UNS N08811, and UNS N08890 are normally employed in service temperatures above 1100°F (593°C) where resistance to creep and rupture is required, and they are annealed to develop controlled grain size for optimum properties in this temperature range.

1.2 The values stated in inch-pound units are to be regarded as the standard. The values given in parentheses are for information only.

1.3 The following safety hazards caveat pertains only to the test method portion, Section 13, of this specification. This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to become familiar with all hazards including those identified in the appropriate Material Safety Data Sheet (MSDS) for this product/material as provided by the manufacturer, to establish appropriate safety and health practices, and determine the applicability of regulatory limitations.

ASTM B407-08 Referenced Document

  • ASTM B880 Standard Specification for General Requirements for Chemical Check Analysis Limits for Nickel, Nickel Alloys, and Cobalt Alloys
  • ASTM E112 Standard Test Methods for Determining Average Grain Size
  • ASTM E140 Standard Hardness Conversion Tables for Metals Relationship Among Brinell Hardness, Vickers Hardness, Rockwell Hardness, Superficial Hardness, Knoop Hardness, and Scleroscope Hardness
  • ASTM E1473 Standard Test Methods for Chemical Analysis of Nickel, Cobalt, and High-Temperature Alloys
  • ASTM E18 Standard Test Methods for Rockwell Hardness of Metallic Materials
  • ASTM E29 Standard Practice for Using Significant Digits in Test Data to Determine Conformance with Specifications
  • ASTM E426 Standard Practice for Electromagnetic (Eddy-Current) Examination of Seamless and Welded Tubular Products, Austenitic Stainless Steel and Similar Alloys
  • ASTM E571 Standard Practice for Electromagnetic (Eddy-Current) Examination of Nickel and Nickel Alloy Tubular Products
  • ASTM E8 Standard Test Methods for Tension Testing of Metallic Materials

ASTM B407-08 history

  • 2022 ASTM B407-22 Standard Specification for Nickel-Iron-Chromium Alloy Seamless Pipe and Tube
  • 2019 ASTM B407-08a(2019) Standard Specification for Nickel-Iron-Chromium Alloy Seamless Pipe and Tube
  • 2008 ASTM B407-08a(2014) Standard Specification for Nickel-Iron-Chromium Alloy Seamless Pipe and Tube
  • 2008 ASTM B407-08a Standard Specification for Nickel-Iron-Chromium Alloy Seamless Pipe and Tube
  • 2008 ASTM B407-08 Standard Specification for Nickel-Iron-Chromium Alloy Seamless Pipe and Tube
  • 2004 ASTM B407-04 Standard Specification for Nickel-Iron-Chromium Alloy Seamless Pipe and Tube
  • 2001 ASTM B407-01 Standard Specification for Nickel-Iron-Chromium Alloy Seamless Pipe and Tube
  • 1996 ASTM B407-96 Standard Specification for Nickel-Iron-Chromium Alloy Seamless Pipe and Tube
Standard Specification for  Nickel-Iron-Chromium Alloy Seamless Pipe and Tube



Copyright ©2024 All Rights Reserved