DIN EN 15361:2007
Determination of the influence of the corrosion protection coating on the anchorage capacity of the transverse anchorage bars in prefabricated reinforced components of autoclaved aerated concrete; English version of DIN EN 15361:2007-06

Standard No.
DIN EN 15361:2007
Release Date
2007
Published By
German Institute for Standardization
Status
Replace By
DIN EN 15361:2007-06
Latest
DIN EN 15361:2007-06
Replace
DIN EN 15361:2005
Scope
This document specifies a pull-out test method for the verification of the applicability of the declared outer diameter of the transverse bars with corrosion protection coating ф in the calculation of the anchorage capacity of transverse anchorage bars (see A.10.3 in prEN 12602-2006) in prefabricated reinforced components of autocalaved aerated concrete(AAC).

DIN EN 15361:2007 Referenced Document

  • EN 678 Determination of the dry density of autoclaved aerated concrete
  • EN 679 Determination of the compressive strength of autoclaved aerated concrete

DIN EN 15361:2007 history

  • 2007 DIN EN 15361:2007-06 Determination of the influence of the corrosion protection coating on the anchorage capacity of the transverse anchorage bars in prefabricated reinforced components of autoclaved aerated concrete; German version EN 15361:2007
  • 2007 DIN EN 15361:2007 Determination of the influence of the corrosion protection coating on the anchorage capacity of the transverse anchorage bars in prefabricated reinforced components of autoclaved aerated concrete; English version of DIN EN 15361:2007-06
  • 0000 DIN EN 15361:2005
Determination of the influence of the corrosion protection coating on the anchorage capacity of the transverse anchorage bars in prefabricated reinforced components of autoclaved aerated concrete; English version of DIN EN 15361:2007-06



Copyright ©2024 All Rights Reserved