SAE AMS5667L-2003
Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 72Ni 15.5Cr 0.95Cb 2.5Ti 0.70Al 7.0Fe Equalized, Precipitation Hardenable

Standard No.
SAE AMS5667L-2003
Release Date
2003
Published By
Society of Automotive Engineers (SAE)
Status
Replace By
SAE AMS5667M-2008
Latest
SAE AMS5667P-2020
Scope
This specification covers a corrosion and heat resistant nickel alloy in the form of bars, forgings, flash welded rings, and stock for forging, flash welded rings, or heading. These products have been used typically for parts, such as bolts and turbine rotors, requiring high strength in the range of 800 to 1100 degrees F (427 to 593 degrees C), but usage is not limited to such applications.

SAE AMS5667L-2003 history

  • 2020 SAE AMS5667P-2020 Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 72Ni - 15.5Cr - 0.95Cb - 2.5Ti - 0.70Al - 7.0Fe Equalized, Precipitation Hardenable
  • 2015 SAE AMS5667N-2015 Nickel Alloy@ Corrosion and Heat-Resistant@ Bars@ Forgings@ and Rings 72Ni - 15.5Cr - 0.95Cb - 2.5Ti - 0.70Al - 7.0Fe Equalized@ Precipitation Hardenable (UNS N07750)
  • 2008 SAE AMS5667M-2008 Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 72Ni-15.5Cr-0.95Cb-2.5Ti-0.70Al-7.0Fe Equalized, Precipitation Hardenable
  • 2003 SAE AMS5667L-2003 Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 72Ni 15.5Cr 0.95Cb 2.5Ti 0.70Al 7.0Fe Equalized, Precipitation Hardenable
  • 1996 SAE AMS5667K-1996 Nickel Alloy@ Corrosion and Heat Resistant@ Bars@ Forgings@ and Rings 72Ni - 15.5Cr - 0.95Cb - 2.5Ti - 0.70Al - 7.0Fe Equalized@ Precipitation Hardenable (UNS N07750)
  • 1990 SAE AMS5667J-1990 Alloy@ Bars@ Forgings@ and Rings Corrosion and Heat Resistant 72Ni - 15.5Cr - 0.95(Cb + Ta) - 2.5Ti - 0.70Al - 7.0Fe Equalized@ Precipitation Hardenable (UNS N07750)
  • 1979 SAE AMS5667H-1979 ALLOY BARS, FORGINGS, AND RINGS, CORROSION AND HEAT RESISTANT 72Ni - 15.5Cr - 0.95(Cb + Ta) - 2.5Ti - 0.70Al - 7.0Fe
  • 1972 SAE AMS5667G-1972 ALLOY BARS, FORGINGS, AND RINGS, CORROSION AND HEAT RESISTANT Nickel Base - 15.5Cr - 7.0Fe - 2.5Ti - 1.0(Cb+Ta) - 0.70Al
  • 1960 SAE AMS5667F-1960 ALLOY, CORROSION AND HEAT RESISTANT Nickel Base - 15.5Cr - 7Fe - 2.5Ti - 1(Cb+Ta) - 0.7Al
  • 1958 SAE AMS5667E-1958 ALLOY, CORROSION AND HEAT TREATMENT Nickel Base - 15.5Cr - 7Fe - 2.5Ti - 1(Cb+Ta) - 0.7Al
  • 1953 SAE AMS5667D-1953 ALLOY, CORROSION AND HEAT RESISTANT Nickel Base - 15.5Cr - 7Fe - 2.5Ti - 1(Cb+Ta) - 0.7Al
  • 1951 SAE AMS5667C-1951 ALLOY, CORROSION AND HEAT RESISTANT Nickel Base - 15Cr - 7Fe - 2.5Ti - 1(Cb+Ta) - 0.7Al
  • 1950 SAE AMS5667B-1950 ALLOY, CORROSION AND HEAT RESISTANT Nickel Base - 15Cr - 7Fe - 2.5Ti - 1Cb - 0.7Al
  • 1949 SAE AMS5667A-1949 ALLOY, CORROSION AND HEAT RESISTANT Nickel Base - 15Cr - 7Fe - 2.5Ti - 1Cb - 0.7Al
  • 1947 SAE AMS5667-1947 ALLOY, CORROSION AND HEAT RESISTANT Nickel Base - 15Cr - 2.5Ti - 1Cb - 0.7Al Precipitation Heat Treated



Copyright ©2024 All Rights Reserved