Scope
This specification covers a corrosion and heat-resistant nickel alloy in the form of bars, forgings, flash welded rings, and stock for forging, flash welded rings. These products have been used typically for parts requiring high resistance to creep and stress-rupture up to 1400 °F (760 °C) and oxidation resistance up to 1800 °F (982 °C), but usage is not limited to such applications.

SAE AMS5442-2006 history

  • 2022 SAE AMS5442B-2022 Nickel Alloy, Corrosion- and Heat-Resistant, Bars, Forgings, and Rings Ni - 18Cr - 2.8Mo - 5.5Cb(Nb) - 0.70Ti - 1.50Al - 10Fe - 9Co - 1W Consumable Electrode Remelted or Vacuum Induction Melted 1775 °F (968 °C) Solution and Precipitation Heat Treated
  • 2017 SAE AMS5442B-2017 Nickel Alloy@ Corrosion and Heat-Resistant@ Bars@ Forgings@ and Rings Ni - 18Cr - 2.8Mo - 5.5Cb(Nb) - 0.70Ti - 1.50Al - 10Fe - 9Co - 1W Consumable Electrode Remelted or Vacuum Induction Melted 1775 °F (968 °C) Solution and Precipitation Heat Treated (UNS
  • 2011 SAE AMS5442A-2011 Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings Ni 18Cr 2.8Mo 5.5Cb(Nb) 0.70Ti 1.50Al 10Fe 9Co 1W Consumable Electrode Remelted or Vacuum Induction Melted 1775 °F (968 °C) Solution and Precipitation Heat Treated
  • 2006 SAE AMS5442-2006 Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings Ni - 18Cr - 2.8Mo - 5.5Cb(Nb) - 0.70Ti - 1.50Al - 10Fe - 9Co - 1W Consumable Electrode Remelted or Vacuum Induction Melted 1775 degrees F (968 degrees C) Solution and Precipitation Hea



Copyright ©2024 All Rights Reserved